Physical Properties | Metric | English | Comments |
|
Density | 1.39 g/cc | 0.0502 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | 0.125 inch; ASTM D 955 |
Melt Flow | 13 g/10 min | 13 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 138 MPa | 20000 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 138 MPa | 20000 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 3 % | 3 % | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Yield | 3 % | 3 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 6.89 GPa | 1000 ksi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 6.89 GPa | 1000 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Modulus | 6.89 GPa | 1000 ksi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Strength | 207 MPa | 30000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Yield Strength | 207 MPa | 30000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 5.87 J/cm | 11 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 14.9 J | 11 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 0.801 J/cm | 1.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | Surface (+/- 0.125 inch); PLC Code 3; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | 3.15 - 5.91 in/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 36 µm/m-°C | 20 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 72 µm/m-°C | 40 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 211 °C | 412 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 0.46 MPa (66 psi) | 214 °C | 417 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 206 °C | 403 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 209 °C | 408 °F | 0.250 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 210 °C | 410 °F | Rate B; ASTM D 1525 |
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.016 in. |
Descriptive Properties |
|
UL File Number, USA | E121562 | |
|
Printer friendly version |