MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics ULTEM 2300 Polyetherimide (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Click here to view available vendors for this material.

Physical PropertiesMetricEnglishComments
Density1.51 g/cc0.0546 lb/in³ ASTM D 792
Water Absorption0.16 %0.16 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.9 %0.9 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.002 - 0.004 cm/cm0.002 - 0.004 in/in Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.002 - 0.004 cm/cm0.002 - 0.004 in/in 0.125 inch; ASTM D 955
Melt Flow5 g/10 min5 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Hardness, Rockwell M114114 ASTM D 785
Tensile Strength @ Break159 MPa23000 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield169 MPa24500 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3 %3 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus9.31 GPa1350 ksi 0.2 in/min; ASTM D 638
Flexural Modulus8.96 GPa1300 ksi 0.10 in/min, 4" span; ASTM D 790
Flexural Strength228 MPa33000 psi 0.10 in/min, 4" span; ASTM D 790
Izod Impact, Unnotched4.27 J/cm8 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.854 J/cm1.6 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched4.91 J/cm9.2 ft-lb/in Reverse Notched, 73F; ASTM D 256

Electrical Properties
Volume Resistivity3e+016 ohm-cm3e+016 ohm-cm ASTM D 257
Dielectric Constant3.73.7 1 kHz; ASTM D 150
Dielectric Strength24.8 kV/mm630 V/mil in air, 62 mils; ASTM D 149
Dielectric Strength30.3 kV/mm770 V/mil in oil, 62 mils; ASTM D 149
Dissipation Factor0.00150.0015 1 kHz; ASTM D 150
Dissipation Factor0.00530.0053 2450 MHz; ASTM D 150
Arc Resistance60 - 120 sec60 - 120 sec Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495
Comparative Tracking Index100 - 175 V100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAIMax 15 arcsMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTR80 - 150 mm/min3.15 - 5.91 in/min (+/- 0.125 inch); PLC Code 3; UL 746A

Thermal Properties
CTE, linear, 212°F (100°C)19.8 µm/m-°C11 µin/in-°F Flow, 0F to 300F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)212 °C414 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)210 °C410 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point228 °C442 °F Rate B; ASTM D 1525
UL RTI, Electrical180 °C356 °F UL 746B
UL RTI, Mechanical with Impact170 °C338 °F UL 746B
UL RTI, Mechanical without Impact180 °C356 °F UL 746B
Flammability, UL94V-0V-0 0.01 in.
Flammability, UL9477 0.048 in.
NBS Smoke Density1.61.6 Flaming, Ds 4 min; ASTM E 662
NBS Smoke Density2020 Flaming, Dmax 20 min; ASTM E 662
NBS Smoke Density2020 Smolder, Dmax 20 min; ASTM E 662
Oxygen Index50 %50 % ASTM D 2863

Descriptive Properties
CSA File No.LS88480 
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。