| Physical Properties | Metric | English | Comments |
|
| Density | 1.61 g/cc | 0.0582 lb/in³ | ASTM D 792 |
| Water Absorption | 0.13 % | 0.13 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 0.9 % | 0.9 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.001 - 0.003 cm/cm | 0.001 - 0.003 in/in | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 4.2 g/10 min | 4.2 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 114 | 114 | ASTM D 785 |
| Tensile Strength @ Break | 179 MPa | 26000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2.5 % | 2.5 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 11.7 GPa | 1700 ksi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 11.7 GPa | 1700 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 241 MPa | 35000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 4.27 J/cm | 8 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1.12 J/cm | 2.1 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 4.81 J/cm | 9 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 1.5e+016 ohm-cm | 1.5e+016 ohm-cm | ASTM D 257 |
| Dielectric Constant | 3.7 | 3.7 | 1 kHz; ASTM D 150 |
| Dielectric Strength | 24 kV/mm | 610 V/mil | in oil, 62 mils; ASTM D 149 |
| Dissipation Factor | 0.002 | 0.002 | 1 kHz; ASTM D 150 |
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | Max 100 V | Max 100 V | (+/- 0.125 inch); PLC Code 5; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | Min 5.91 in/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
| CTE, linear, 212°F (100°C) | 14.4 µm/m-°C | 8 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 234 °C | 454 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | 338 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.01 in. |
| NBS Smoke Density | 1 | 1 | Flaming, Ds 4 min; ASTM E 662 |
| NBS Smoke Density | 20 | 20 | Smolder, Dmax 20 min; ASTM E 662 |
| Oxygen Index | 54 % | 54 % | ASTM D 2863 |
Descriptive Properties |
|
| CSA File No. | LS88480 | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |