SABIC Innovative Plastics ULTEM 4000 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D 792 |
| Water Absorption | 0.11 % | 0.11 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | 0.002 - 0.003 in/in | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 3.1 g/10 min | 3.1 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 85 | 85 | ASTM D 785 |
| Tensile Strength @ Break | 82.7 MPa | 12000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 1.2 % | 1.2 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 8.83 GPa | 1280 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 138 MPa | 20000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 114 MPa | 16500 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 1.6 J/cm | 3 ft-lb/in | 73F; ASTM D 4812 |
| Coefficient of Friction | 0.24 | 0.24 | Vs. Steel, Kinetic; ASTM D 1894 |
| Coefficient of Friction, Static | 0.25 | 0.25 | Vs. Steel; ASTM D 1894 |
| K (wear) Factor | 3830 x 10-8 mm³/N-M | 1900 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; GE Test |
| K (wear) Factor | 125 x 10-8 mm³/N-M | 62 x 10-10 in³-min/ft-lb-hr | PV = 2000 psi-fpm vs Steel; GE Test |
| Limiting Pressure Velocity | 2.1 MPa-m/sec | 60000 psi-ft/min | 100 fpm; GE Test |
| Taber Abrasion, mg/1000 Cycles | 33 | 33 | CS-17, 1 kg; ASTM D 1044 |
| Izod Impact, Notched | 0.641 J/cm | 1.2 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 1.71 J/cm | 3.2 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
| CTE, linear 68°F | 16.2 µm/m-°C | 9 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 16.2 µm/m-°C | 9 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 212 °C | 414 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 234 °C | 453 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
| UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
| UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.033 in. |
Descriptive Properties | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|