SABIC Innovative Plastics VALOX CS860 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | 0.002 - 0.003 in/in | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.005 - 0.006 cm/cm | 0.005 - 0.006 in/in | 0.125 inch; ASTM D 955 |
Melt Flow | 45 g/10 min | 45 g/10 min | 266C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 110 MPa | 16000 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 108 MPa | 15700 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 3.1 % | 3.1 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 6.21 GPa | 900 ksi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 8.27 GPa | 1200 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 155 MPa | 22500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 5.34 J/cm | 10 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 0.801 J/cm | 1.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | Min 5.91 in/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 188 °C | 370 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.03 in. |
Flammability, UL94 | 7 | 7 | 0.118 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|