MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

SABIC Innovative Plastics VALOX DR51U PBT (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.41 g/cc0.0509 lb/in³ ASTM D 792
Water Absorption0.07 %0.07 % 24 hours @ 73F; ASTM D 570
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow, 60-125 mil; ASTM D 955
Linear Mold Shrinkage0.006 - 0.009 cm/cm0.006 - 0.009 in/in Flow, 125-180 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.008 cm/cm0.005 - 0.008 in/in 60-125 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.008 - 0.011 cm/cm0.008 - 0.011 in/in 125-180 mil; ASTM D 955

Mechanical Properties
Hardness, Rockwell R118118 ASTM D 785
Tensile Strength @ Break93.1 MPa13500 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break5 %5 % Type I, 0.2 in/min; ASTM D 638
Flexural Modulus4.83 GPa700 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength145 MPa21000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched5.34 J/cm10 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.534 J/cm1 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume Resistivity3.3e+016 ohm-cm3.3e+016 ohm-cm ASTM D 257
Dielectric Constant3.43.4 1 MHz; ASTM D 150
Dielectric Constant3.63.6 100 Hz; ASTM D 150
Dielectric Strength19.7 kV/mm500 V/mil in air, 125 mils; ASTM D 149
Dielectric Strength23.2 kV/mm590 V/mil in oil, 62 mils; ASTM D 149
Dissipation Factor0.0020.002 100 Hz; ASTM D 150
Dissipation Factor0.020.02 1 MHz; ASTM D 150
Arc Resistance120 - 180 sec120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index250 - 400 V250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
High Voltage Arc-Tracking Rate, HVTR10 - 25.4 mm/min0.394 - 1 in/min (+/- 0.125 inch); PLC Code 1; UL 746A

Thermal Properties
CTE, linear 68°F21.6 µm/m-°C12 µin/in-°F Flow, -40F to 200F; ASTM E 831
CTE, linear, 212°F (100°C)21.6 µm/m-°C12 µin/in-°F Flow, 140F to 280F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)210 °C410 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)191 °C375 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical130 °C266 °F UL 746B
UL RTI, Mechanical with Impact130 °C266 °F UL 746B
UL RTI, Mechanical without Impact140 °C284 °F UL 746B
Flammability, UL94HBHB 0.028 in.

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。