SABIC Innovative Plastics VALOX FV620 PBT (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.46 g/cc0.0527 lb/in³ Molded Foam; ASTM D 792
Density1.62 g/cc0.0585 lb/in³ ASTM D 792
Water Absorption0.04 %0.04 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.09 %0.09 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.003 - 0.005 cm/cm0.003 - 0.005 in/in Flow, 0.250 inch; ASTM D 955

Mechanical Properties
Tensile Strength @ Yield77.2 MPa11200 psi 0.250"; ASTM D 638
Elongation at Break4.8 %4.8 % 0.250"; ASTM D 638
Tensile Modulus8.38 GPa1215 ksi 0.250"; ASTM D 638
Flexural Modulus7.65 GPa1110 ksi 0.250"; ASTM D 790
Flexural Yield Strength147 MPa21300 psi 0.250"; ASTM D 790
Izod Impact, Unnotched5.34 J/cm10 ft-lb/in 73F; ASTM D 4812
Falling Dart Impact14.9 J11 ft-lb 73F; GE Test

Electrical Properties
Volume Resistivity2.5e+017 ohm-cm2.5e+017 ohm-cm ASTM D 257
Surface Resistivity per SquareMin 1.1e+017 ohmMin 1.1e+017 ohm ASTM D 257
Dielectric Constant2.942.94 1 MHz; ASTM D 150
Dielectric Constant3.093.09 100 Hz; ASTM D 150
Dissipation Factor0.0040.004 100 Hz; ASTM D 150
Dissipation Factor0.0110.011 1 MHz; ASTM D 150
Arc ResistanceMax 60 secMax 60 sec Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495
Comparative Tracking Index175 - 250 V175 - 250 V (+/- 0.125 inch); PLC Code 3; UL 746A
Hot Wire Ignition, HWI30 - 60 sec30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAI30 - 60 arcs30 - 60 arcs Surface (+/- 0.125 inch); PLC Code 2; UL 746A
High Voltage Arc-Tracking Rate, HVTR25.4 - 80 mm/min1 - 3.15 in/min (+/- 0.125 inch); PLC Code 2; UL 746A

Thermal Properties
CTE, linear 68°F23.4 µm/m-°C13 µin/in-°F Flow, -40F to 200F; ASTM E 831
Specific Heat Capacity1.15 J/g-°C0.276 BTU/lb-°F ASTM C 351
Thermal Conductivity0.16 W/m-K1.11 BTU-in/hr-ft²-°F ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)202 °C395 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)141 °C285 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical75 °C167 °F UL 746B
UL RTI, Mechanical with Impact75 °C167 °F UL 746B
UL RTI, Mechanical without Impact75 °C167 °F UL 746B
Flammability, UL94V-0V-0 0.154 in.
Flammability, UL9477 0.193 in.
Flammability Test1.21.2 FOAM - Flame Class Minimum Density; g/cm3

Descriptive Properties
Foam Weight Reduction10% Mechanical Properties Reported Herein (0.250")
Foam Weight Reduction10% Impact Properties Reported Herein (0.250")
Foam Weight Reduction10% Thermal Properties Reported Herein (0.250")
Foam Weight Reduction10% Physical Properties Reported Herein (0.250")
Foam Weight Reduction20% Electrical Properties Reported Herein (0.250")
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。