SABIC Innovative Plastics VALOX HF4030 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic 
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics. 
Material Notes:  Information provided by GE Plastics for their North American product line. 
| Physical Properties | Metric | English | Comments |  
 |  
| Density | 1.51 g/cc | 0.0546 lb/in³ |  ASTM D 792 |  
| Water Absorption | 0.037 % | 0.037 % |  24 hours @ 73F; ASTM D 570 |  
| Viscosity | 470000 cP | 470000 cP |  Melt Viscosity; GE Test |  
| Linear Mold Shrinkage | 0.005 cm/cm | 0.005 in/in |  Flow, 0.125 inch; ASTM D 955 |  
| Linear Mold Shrinkage, Transverse | 0.009 cm/cm | 0.009 in/in |  0.125 inch; ASTM D 955 |  
 Mechanical Properties |  
 |  
| Tensile Strength @ Break | 105 MPa | 15200 psi |  Type I, 0.2 in/min; ASTM D 638 |  
| Elongation at Break | 2 % | 2 % |  Type I, 0.2 in/min; ASTM D 638 |  
| Flexural Modulus | 7.24 GPa | 1050 ksi |  0.05 in/min, 2" span; ASTM D 790 |  
| Flexural Strength | 190 MPa | 27500 psi |  0.05 in/min, 2" span; ASTM D 790 |  
| Izod Impact, Unnotched | 7.21 J/cm | 13.5 ft-lb/in |  73F; ASTM D 4812 |  
| Izod Impact, Notched | 0.801 J/cm | 1.5 ft-lb/in |  73F; ASTM D 256 |  
 Electrical Properties |  
 |  
| Volume Resistivity | Min 1e+016 ohm-cm | Min 1e+016 ohm-cm |  ASTM D 257 |  
| Dielectric Constant | 3.1 | 3.1 |  1 MHz; ASTM D 150 |  
| Dielectric Strength | 18.5 kV/mm | 471 V/mil |  in oil, 125 mils; ASTM D 149 |  
| Dissipation Factor | 0.01 | 0.01 |  1 MHz; ASTM D 150 |  
| Arc Resistance | 120 - 180 sec | 120 - 180 sec |  Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |  
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V |  (+/- 0.125 inch); PLC Code 1; UL 746A |  
| Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec |  (+/- 0.125 inch); PLC Code 0; UL 746A |  
| High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs |  Surface (+/- 0.125 inch); PLC Code 0; UL 746A |  
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min |  (+/- 0.125 inch); PLC Code 2; UL 746A |  
 Thermal Properties |  
 |  
| CTE, linear 68°F | 27 µm/m-°C | 15 µin/in-°F |  Flow, -40F to 100F; ASTM E 831 |  
| CTE, linear 68°F, Transverse to Flow | 79.2 µm/m-°C | 44 µin/in-°F |  from -40F to 100F; ASTM E 831 |  
| CTE, linear, 212°F (100°C) | 23.4 µm/m-°C | 13 µin/in-°F |  Flow, 140F to 280F; ASTM E 831 |  
| CTE, linear, 212°F (100°C) | 160 µm/m-°C | 89 µin/in-°F |  Cross Flow, 140F to 280F; ASTM E 831 |  
| Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F |  0.250 inch, unannealed; ASTM D 648 |  
| UL RTI, Electrical | 140 °C | 284 °F |  UL 746B |  
| UL RTI, Mechanical with Impact | 140 °C | 284 °F |  UL 746B |  
| UL RTI, Mechanical without Impact | 140 °C | 284 °F |  UL 746B |  
| Flammability, UL94 | HB | HB |  0.03 in. |  
 Descriptive Properties |   |  
| UL File Number, USA | E121562 |   |  
 |  
  Printer friendly version |  
 
   Some of the values displayed above may have been converted from their original units and/or rounded in
  order to display the information in a consistant format.  Users requiring more precise data for scientific or
  engineering calculations can click on the property value to see the original value as well as raw conversions
  to equivalent units.  We advise that you only use the original value or one of its raw conversions in your
  calculations to minimize rounding error.  We also ask that you refer to MatWeb's disclaimer and terms of use
  regarding this information.  Click here to
  view all the property values for this datasheet as they were originally entered into MatWeb. 
     
  
  
   |