SABIC Innovative Plastics VALOX V3001MC PBT (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesMetricEnglishComments
Density1.31 g/cc0.0473 lb/in³ ISO 1183
Density1.32 g/cc0.0477 lb/in³ ASTM D 792
Water Absorption0.08 %0.08 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.34 %0.34 % 73F; ASTM D 570
Linear Mold Shrinkage0.018 - 0.021 cm/cm0.018 - 0.021 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow30 g/10 min30 g/10 min Melt Volume Rate, MVR at 250C/2.16 kg; cm3/10min; ISO 1133
Melt Flow33 g/10 min33 g/10 min 250C/2.16 kgf; ASTM D 1238

Mechanical Properties
Hardness, Rockwell R117117 ISO 2039/2
Tensile Strength, Ultimate53 MPa7690 psi 50 mm/min; ISO 527
Tensile Strength @ Break17.9 MPa2600 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength, Yield59 MPa8560 psi 50 mm/min; ISO 527
Tensile Strength @ Yield55.2 MPa8000 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break100 %100 % Type I, 2.0 in/min; ASTM D 638
Elongation at Break15 %15 % 50 mm/min; ISO 527
Elongation at Yield20 %20 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield7 %7 % 50 mm/min; ISO 527
Tensile Modulus2.7 GPa392 ksi 1 mm/min; ISO 527
Tensile Modulus2.65 GPa385 ksi 2.0 in/min; ASTM D 638
Flexural Modulus2.6 GPa377 ksi 2 mm/min; ISO 178
Flexural Modulus2.41 GPa350 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength90 MPa13100 psi 2 mm/min; ISO 178
Flexural Yield Strength89.6 MPa13000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)NBNB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NBNB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4; -30 C; ISO 180/ 1A
Izod Impact, Notched, Low Temp0.587 J/cm1.1 ft-lb/in at -40F; ASTM D 256
Charpy Impact UnnotchedNBNB 23C, Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.3 J/cm²1.43 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB at -30C, Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched0.3 J/cm²1.43 ft-lb/in² 23 C; ISO 179/2C
Charpy Impact, Notched0.6 J/cm²2.86 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Gardner Impact @ 23°C56.6 J41.7 ft-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched0.427 J/cm0.8 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm IEC 60093
Dielectric Constant3.13.1 1 MHz; IEC 60250
Dielectric Constant3.33.3 50 Hz; IEC 60250
Dielectric Strength18 kV/mm457 kV/in in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.0020.002 50 Hz; IEC 60250
Dissipation Factor0.020.02 1 MHz; IEC 60250
Comparative Tracking Index600 V600 V IEC 112/3rd

Thermal Properties
CTE, linear 20°C130 µm/m-°C72.2 µin/in-°F Flow, 23C-80C; ISO 11359-2
CTE, linear 20°C Transverse to Flow130 µm/m-°C72.2 µin/in-°F 23C-80C; ISO 11359-2
Thermal Conductivity0.16 W/m-K1.11 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)160 °C320 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)154 °C309 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 0.46 MPa (66 psi)174 °C345 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point185 °C365 °F B/50; ISO 306
Vicat Softening Point185 °C365 °F B/120; ISO 306
Vicat Softening Point185 °C365 °F Rate B; ASTM D 1525
Oxygen Index20 %20 % ISO 4589

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Hardness, H358/30 (MPa)85 ISO 2039/1
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。