SABIC Innovative Plastics VALOX 508 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
Physical Properties | Metric | English | Comments |
|
Density | 1.5 g/cc | 0.0542 lb/in³ | ASTM D 792 |
Water Absorption | 0.06 % | 0.06 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | Flow, 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow, 125-180 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 0.006 - 0.009 in/in | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
Hardness, Rockwell R | 119 | 119 | ASTM D 785 |
Tensile Strength @ Break | 110 MPa | 16000 psi | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 6.89 GPa | 1000 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 190 MPa | 27500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 6.41 J/cm | 12 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched, Low Temp | 0.801 J/cm | 1.5 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 6.78 J | 5 ft-lb | Instrumented Impact Energy @ peak, 73°F; ASTM D 3763 |
Gardner Impact @ 23°C | 8.13 J | 6 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 0.961 J/cm | 1.8 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | 5.9e+016 ohm-cm | 5.9e+016 ohm-cm | ASTM D 257 |
Dielectric Constant | 3.6 | 3.6 | 100 Hz; ASTM D 150 |
Dielectric Constant | 3.6 | 3.6 | 1 MHz; ASTM D 150 |
Dielectric Strength | 23.6 kV/mm | 600 V/mil | in air, 125 mils; ASTM D 149 |
Dielectric Strength | 29.1 kV/mm | 740 V/mil | in oil, 62 mils; ASTM D 149 |
Dissipation Factor | 0.0014 | 0.0014 | 100 Hz; ASTM D 150 |
Dissipation Factor | 0.02 | 0.02 | 1 MHz; ASTM D 150 |
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | Surface (+/- 0.125 inch); PLC Code 3; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 23.4 µm/m-°C | 13 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear, 212°F (100°C) | 16.2 µm/m-°C | 9 µin/in-°F | Flow, 140F to 280F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 177 °C | 350 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
Flammability, UL94 | HB | HB | 0.058 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F2 | UL746C |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|