SABIC Innovative Plastics ULTEM AR9300 Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D 792 |
| Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | Flow; ASTM D 955 |
| Melt Flow | 6 g/10 min | 6 g/10 min | cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133 |
Mechanical Properties |
|
| Hardness, H358/30 | 160 MPa | 23200 psi | ISO 2039/1 |
| Tensile Strength, Ultimate | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 2 % | 2 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 9.5 GPa | 1380 ksi | 1 mm/min; ISO 527 |
| Flexural Modulus | 8.5 GPa | 1230 ksi | 2 mm/min; ISO 178 |
| Flexural Yield Strength | 225 MPa | 32600 psi | 2 mm/min; ISO 178 |
| Izod Impact, Unnotched (ISO) | 35 kJ/m² | 16.7 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1U |
| Izod Impact, Unnotched Low Temp (ISO) | 35 kJ/m² | 16.7 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1U |
| Charpy Impact Unnotched | 4 J/cm² | 19 ft-lb/in² | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
| Charpy Impact, Unnotched Low Temp | 4 J/cm² | 19 ft-lb/in² | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Thermal Properties |
|
| CTE, linear 100°C | 17 µm/m-°C | 9.44 µin/in-°F | 23C-150C, flow; ISO 11359-2 |
| CTE, linear 100°C | 42 µm/m-°C | 23.3 µin/in-°F | 23C-150C, cross flow; ISO 11359-2 |
| Thermal Conductivity | 0.29 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 212 °C | 414 °F | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 208 °C | 406 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 210 °C | 410 °F | B/50; ISO 306 |
| Vicat Softening Point | 215 °C | 419 °F | B/120; ISO 306 |
| Vicat Softening Point | 220 °C | 428 °F | A/50; ISO 306 |
| Flammability Test | 40 | 40 | KW/m2; OSU peak heat, release rate; FAR 25.853 |
| Flammability Test | 5 | 5 | KW-min/m2; OSU 2 minute heat, release rate; FAR 25.853 |
| NBS Smoke Density | 5 | 5 | Flaming, Ds 4 min; ASTM E 662 |
| NBS Smoke Density | 5 | 5 | Flaming, Dmax 20 min; ASTM E 662 |
Descriptive Properties | |
| Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|