COMSOL CD

SABIC Innovative Plastics ULTEM ATX100F Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesMetricEnglishComments
Density1.21 g/cc0.0437 lb/in³ ASTM D 792
Density1.21 g/cc0.0437 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.25 %0.25 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.5 %0.5 % 23C; ISO 62
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow; ASTM D 955
Melt Flow35 g/10 min35 g/10 min cm3/10min; Melt Volume Rate, MVR at 340C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/3095 MPa13800 psi ISO 2039/1
Tensile Strength, Ultimate55 MPa7980 psi 50 mm/min; ISO 527
Tensile Strength, Yield65 MPa9430 psi 50 mm/min; ISO 527
Elongation at Break30 %30 % 50 mm/min; ISO 527
Elongation at Yield7 %7 % 50 mm/min; ISO 527
Tensile Modulus2.35 GPa341 ksi 1 mm/min; ISO 527
Flexural Modulus2.4 GPa348 ksi 2 mm/min; ISO 178
Flexural Yield Strength90 MPa13100 psi 2 mm/min; ISO 178
Izod Impact, Notched (ISO)15 kJ/m²7.14 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Notched, Low Temp (ISO)13 kJ/m²6.19 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact, Notched, Low Temp1.5 J/cm²7.14 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Notched1.9 J/cm²9.04 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.82.8 1 MHz; IEC 60250
Dielectric Constant2.92.9 50 Hz; IEC 60250
Dielectric Strength22 kV/mm559 kV/in in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.0010.001 50 Hz; IEC 60250
Dissipation Factor0.0130.013 1 MHz; IEC 60250
Comparative Tracking Index175 V175 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C60 µm/m-°C33.3 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C60 µm/m-°C33.3 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.24 W/m-K1.67 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)160 °C320 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)150 °C302 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point170 °C338 °F B/50; ISO 306
Vicat Softening Point175 °C347 °F B/120; ISO 306
Vicat Softening Point180 °C356 °F A/50; ISO 306
Vicat Softening Point187 °C369 °F Rate B; ASTM D 1525
Flammability, UL94HBHB 0.75 mm
Flammability, UL94HBHB 0.75 mm; UL 94 by GE

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。