SABIC Innovative Plastics ULTEM CRS5311 Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.52 g/cc0.0549 lb/in³ ASTM D 792
Density1.52 g/cc0.0549 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.15 %0.15 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.9 %0.9 % 23C; ISO 62
Linear Mold Shrinkage0.002 - 0.004 cm/cm0.002 - 0.004 in/in Flow; ASTM D 955
Melt Flow7 g/10 min7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30165 MPa23900 psi ISO 2039/1
Tensile Strength, Ultimate160 MPa23200 psi 5 mm/min; ISO 527
Elongation at Break2 %2 % 5 mm/min; ISO 527
Tensile Modulus10 GPa1450 ksi 1 mm/min; ISO 527
Flexural Modulus8.2 GPa1190 ksi 2 mm/min; ISO 178
Flexural Strength210 MPa30500 psi 2 mm/min; ISO 178
Compressive Modulus8.3 GPa1200 ksi DIN 53454
Izod Impact, Unnotched (ISO)35 kJ/m²16.7 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)35 kJ/m²16.7 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.13.1 1 MHz; IEC 60250
Dielectric Constant3.23.2 50 Hz; IEC 60250
Dielectric Strength18 kV/mm457 kV/in in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.0020.002 50 Hz; IEC 60250
Dissipation Factor0.0030.003 1 MHz; IEC 60250
Comparative Tracking Index100 V100 V M; IEC 60112/3rd
Comparative Tracking Index150 V150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C20 µm/m-°C11.1 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C70 µm/m-°C38.9 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.33 W/m-K2.29 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)215 °C419 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)215 °C419 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point220 °C428 °F B/120; ISO 306
Vicat Softening Point228 °C442 °F A/50; ISO 306
UL RTI, Electrical105 °C221 °F UL 746B
UL RTI, Mechanical with Impact105 °C221 °F UL 746B
UL RTI, Mechanical without Impact105 °C221 °F UL 746B
Flammability, UL94V-0V-0 1.5 mm
Flammability, UL9477 94-1.5 mm
Flammability Test11 mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; EDF HN60S02
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。