SABIC Innovative Plastics ULTEM SILTEM-STM1500 Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D 792 |
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Water Absorption at Saturation | 0.12 % | 0.12 % | 23C; ISO 62 |
| Linear Mold Shrinkage | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | Flow; ASTM D 955 |
| Melt Flow | 8 g/10 min | 8 g/10 min | cm3/10min; Melt Volume Rate, MVR at 320C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
| Hardness, Shore D | 69 | 69 | DIN 53505 |
| Tensile Strength, Ultimate | 25 MPa | 3630 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 20 MPa | 2900 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 110 % | 110 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 15 % | 15 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 0.59 GPa | 85.6 ksi | 1 mm/min; ISO 527 |
| Flexural Modulus | 0.475 GPa | 68.9 ksi | 2 mm/min; ISO 178 |
| Flexural Strength | 18 MPa | 2610 psi | 2 mm/min; ISO 178 |
| Flexural Yield Strength | 20 MPa | 2900 psi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 25 kJ/m² | 11.9 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1A |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4 +23 C; ISO 180/ 1U |
| Izod Impact, Unnotched Low Temp (ISO) | NB | NB | 80*10*4 -30 C; ISO 180/ 1U |
| Izod Impact, Notched, Low Temp (ISO) | 15 kJ/m² | 7.14 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1A |
| Taber Abrasion, mg/1000 Cycles | 60 | 60 | CS-17, 1 kg; GE Test |
Electrical Properties |
|
| Volume Resistivity | 4.7e+014 ohm-cm | 4.7e+014 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
| Dielectric Constant | 3 | 3 | 100 Hz; IEC 60250 |
| Dielectric Strength | 19 kV/mm | 483 kV/in | in oil, 3.2 mm; IEC 60243-1 |
| Dissipation Factor | 0.0091 | 0.0091 | 100 Hz; IEC 60250 |
| Comparative Tracking Index | 100 V | 100 V | M; IEC 60112/3rd |
| Comparative Tracking Index | 175 V | 175 V | IEC 60112/3rd |
Thermal Properties |
|
| CTE, linear 20°C | 110 µm/m-°C | 61.1 µin/in-°F | 23C-80C, flow; ISO 11359-2 |
| CTE, linear 20°C Transverse to Flow | 90 µm/m-°C | 50 µin/in-°F | 23C-80C; ISO 11359-2 |
| Vicat Softening Point | 75 °C | 167 °F | VST/B/50; DIN 53460 |
| Vicat Softening Point | 75 °C | 167 °F | B/50; ISO 306 |
| Vicat Softening Point | 78 °C | 172 °F | B/120; ISO 306 |
| Flammability, UL94 | V-1 | V-1 | 1.6 mm; UL 94 by GE |
| Oxygen Index | 48 % | 48 % | ISO 4589 |
| Glow Wire Test | 960 °C | 1760 °F | Passes at 3.2 mm; IEC 60695-2-1 |
Descriptive Properties | |
| Ball Pressure Test, 75 C +/- 2 C | PASSES | IEC 60035-1 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|