Physical Properties | Metric | English | Comments |
|
Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D 792 |
Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
Filler Content | 10 % | 10 % | ASTM D 229 |
Water Absorption | 0.28 % | 0.28 % | 24 hours; ASTM D 570 |
Moisture Absorption at Equilibrium | 0.6 % | 0.6 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 1 % | 1 % | 23C; ISO 62 |
Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | Flow; ASTM D 955 |
Melt Flow | 9 g/10 min | 9 g/10 min | cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Rockwell M | 109 | 109 | ISO 2039/2 |
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039/1 |
Tensile Strength, Ultimate | 115 MPa | 16700 psi | ASTM D 638 |
Tensile Strength, Ultimate | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D 638 |
Elongation at Break | 4 % | 4 % | 5 mm/min; ISO 527 |
Elongation at Break | 6 % | 6 % | ASTM D 638 |
Elongation at Yield | 5 % | 5 % | ASTM D 638 |
Tensile Modulus | 4.5 GPa | 653 ksi | DIN 53457 |
Tensile Modulus | 4.5 GPa | 653 ksi | 1 mm/min; ISO 527 |
Flexural Modulus | 4.5 GPa | 653 ksi | DIN 53457 |
Flexural Modulus | 4.5 GPa | 653 ksi | 2 mm/min; ISO 178 |
Flexural Strength | 185 MPa | 26800 psi | 2 mm/min; ISO 178 |
Flexural Strength | 200 MPa | 29000 psi | DIN 53452 |
Ultimate Compressive Strength | 160 MPa | 23200 psi | ASTM D 695 |
Compressive Modulus | 4 GPa | 580 ksi | DIN 53454 |
Poisson's Ratio | 0.38 | 0.38 | ASTM D 638 |
Shear Strength | 90 MPa | 13100 psi | ASTM D 732 |
Izod Impact, Notched | 0.6 J/cm | 1.12 ft-lb/in | 23 C; ASTM D 256 |
Izod Impact, Unnotched | 4.8 J/cm | 8.99 ft-lb/in | 23 C; ASTM D 4812 |
Izod Impact, Unnotched (ISO) | 30 kJ/m² | 14.3 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | 30 kJ/m² | 14.3 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1U |
Charpy Impact, Notched | 0.7 J/cm² | 3.33 ft-lb/in² | 23 C; ISO 179/2C |
Taber Abrasion, mg/1000 Cycles | 15 | 15 | CS-17, 1 kg; GE Test |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.9 | 2.9 | 1 MHz; IEC 60250 |
Dielectric Constant | 3 | 3 | 50 Hz; IEC 60250 |
Dielectric Constant | 3.1 | 3.1 | 60 Hz; IEC 60250 |
Dielectric Strength | 15 kV/mm | 381 kV/in | in oil, 3.2 mm; IEC 60243-1 |
Dielectric Strength | 27 kV/mm | 686 kV/in | in oil, 1.6 mm; IEC 60243-1 |
Dielectric Strength | 34 kV/mm | 864 kV/in | in oil, 0.8 mm; IEC 60243-1 |
Dissipation Factor | 0.0009 | 0.0009 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.0025 | 0.0025 | 1 MHz; IEC 60250 |
Dissipation Factor | 0.0046 | 0.0046 | 2450 MHz; IEC 60250 |
Arc Resistance | 85 sec | 85 sec | Tungsten; ASTM D 495 |
Comparative Tracking Index | 100 V | 100 V | M; IEC 60112/3rd |
Comparative Tracking Index | 150 V | 150 V | IEC 60112/3rd |
Comparative Tracking Index | 150 V | 150 V | Stand. Black; IEC 60112/3rd |
Thermal Properties |
|
CTE, linear 100°C | 26 µm/m-°C | 14.4 µin/in-°F | 23C-150C, flow; ISO 11359-2 |
CTE, linear 100°C | 60 µm/m-°C | 33.3 µin/in-°F | 23C-150C, cross flow; ISO 11359-2 |
Thermal Conductivity | 0.24 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D 648 |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Deflection Temperature at 1.8 MPa (264 psi) | 207 °C | 405 °F | ASTM D 648 |
Vicat Softening Point | 212 °C | 414 °F | B/50; ISO 306 |
Vicat Softening Point | 217 °C | 423 °F | B/120; ISO 306 |
Vicat Softening Point | 223 °C | 433 °F | Rate B; ASTM D 1525 |
Vicat Softening Point | 223 °C | 433 °F | VST/A/120; DIN 53460 |
Vicat Softening Point | 223 °C | 433 °F | A/50; ISO 306 |
UL RTI, Electrical | 170 °C | 338 °F | UL 746B |
UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
UL RTI, Mechanical without Impact | 170 °C | 338 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.41 mm |
Flammability, UL94 | 7 | 7 | 94-1.9 mm |
Flammability Test | 1 | 1 | mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2 |
NBS Smoke Density | 1.8 | 1.8 | Flaming, Ds 4 min; ASTM E 662 |
NBS Smoke Density | 27 | 27 | Flaming, Dmax 20 min; ASTM E 662 |
Oxygen Index | 46 % | 46 % | ISO 4589 |
Glow Wire Test | 960 °C | 1760 °F | Passes at 3.2 mm; EDF HN60S02 |
Glow Wire Test | 960 °C | 1760 °F | Passes at 3.2 mm; IEC 60695-2-1 |
Descriptive Properties |
|
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
Hot Mandrel Test, 300 C | PASSES | CEE10/IIed |
MPa; Hardness, H961/30 | 240 | DIN 53456 |
Needle Flame Test, 3.2 mm, Burn Time s | PASSES | IEC 60695-2-2 |
|
Printer friendly version |