MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics ULTEM 2110 Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.34 g/cc0.0484 lb/in³ ASTM D 792
Density1.34 g/cc0.0484 lb/in³ ISO 1183
Water Absorption0.28 %0.28 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.6 %0.6 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1 %1 % 23C; ISO 62
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow; ASTM D 955
Melt Flow13 g/10 min13 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell M109109 ISO 2039/2
Hardness, H358/30140 MPa20300 psi ISO 2039/1
Tensile Strength, Ultimate115 MPa16700 psi 5 mm/min; ISO 527
Tensile Strength, Ultimate115 MPa16700 psi ASTM D 638
Tensile Strength, Yield120 MPa17400 psi ASTM D 638
Elongation at Break4 %4 % 5 mm/min; ISO 527
Elongation at Break6 %6 % ASTM D 638
Elongation at Yield5 %5 % ASTM D 638
Tensile Modulus4.5 GPa653 ksi DIN 53457
Tensile Modulus4.5 GPa653 ksi 1 mm/min; ISO 527
Flexural Modulus4.5 GPa653 ksi DIN 53457
Flexural Modulus4.5 GPa653 ksi 2 mm/min; ISO 178
Flexural Strength185 MPa26800 psi 2 mm/min; ISO 178
Ultimate Compressive Strength160 MPa23200 psi ASTM D 695
Compressive Modulus4 GPa580 ksi DIN 53454
Shear Strength90 MPa13100 psi ASTM D 732
Izod Impact, Notched0.6 J/cm1.12 ft-lb/in 23 C; ASTM D 256
Izod Impact, Unnotched4.8 J/cm8.99 ft-lb/in 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)30 kJ/m²14.3 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)30 kJ/m²14.3 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U
Charpy Impact Unnotched3.5 J/cm²16.7 ft-lb/in² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Unnotched Low Temp3.5 J/cm²16.7 ft-lb/in² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched0.7 J/cm²3.33 ft-lb/in² 23 C; ISO 179/2C
Taber Abrasion, mg/1000 Cycles1515 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.92.9 1 MHz; IEC 60250
Dielectric Constant33 50 Hz; IEC 60250
Dielectric Strength15 kV/mm381 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength27 kV/mm686 kV/in in oil, 1.6 mm; IEC 60243-1
Dielectric Strength34 kV/mm864 kV/in in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.00090.0009 50 Hz; IEC 60250
Dissipation Factor0.00250.0025 1 MHz; IEC 60250
Dissipation Factor0.00460.0046 2450 MHz; IEC 60250
Arc Resistance85 sec85 sec Tungsten; ASTM D 495
Comparative Tracking Index100 V100 V M; IEC 60112/3rd
Comparative Tracking Index150 V150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C26 µm/m-°C14.4 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C60 µm/m-°C33.3 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.24 W/m-K1.67 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)210 °C410 °F ASTM D 648
Deflection Temperature at 0.46 MPa (66 psi)210 °C410 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)205 °C401 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)207 °C405 °F ASTM D 648
Vicat Softening Point212 °C414 °F B/50; ISO 306
Vicat Softening Point217 °C423 °F B/120; ISO 306
Vicat Softening Point223 °C433 °F Rate B; ASTM D 1525
Vicat Softening Point223 °C433 °F A/50; ISO 306
UL RTI, Electrical170 °C338 °F UL 746B
UL RTI, Mechanical with Impact170 °C338 °F UL 746B
UL RTI, Mechanical without Impact170 °C338 °F UL 746B
Flammability, UL94V-0V-0 0.41 mm
Flammability, UL9477 94-1.9 mm
NBS Smoke Density1.81.8 Flaming, Ds 4 min; ASTM E 662
NBS Smoke Density2727 Flaming, Dmax 20 min; ASTM E 662
Oxygen Index46 %46 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
MPa; Hardness, H961/30240 DIN 53456
Needle Flame Test, 3.2 mm, Burn Time sPASSES IEC 60695-2-2
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。