MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics ULTEM 6000 Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.3 g/cc0.047 lb/in³ ASTM D 792
Density1.3 g/cc0.047 lb/in³ ISO 1183
Water Absorption0.28 %0.28 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.8 %0.8 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1 %1 % 23C; ISO 62
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow; ASTM D 955
Melt Flow7 g/10 min7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30160 MPa23200 psi ISO 2039/1
Tensile Strength, Ultimate95 MPa13800 psi 50 mm/min; ISO 527
Tensile Strength, Yield103 MPa14900 psi ASTM D 638
Elongation at Break30 %30 % ASTM D 638
Elongation at Break4 %4 % 50 mm/min; ISO 527
Elongation at Yield8 %8 % ASTM D 638
Tensile Modulus3 GPa435 ksi DIN 53457
Tensile Modulus3.3 GPa479 ksi 1 mm/min; ISO 527
Flexural Modulus3 GPa435 ksi DIN 53457
Flexural Modulus3.1 GPa450 ksi 2 mm/min; ISO 178
Flexural Yield Strength140 MPa20300 psi 2 mm/min; ISO 178
Flexural Yield Strength145 MPa21000 psi DIN 53452
Ultimate Compressive Strength140 MPa20300 psi ASTM D 695
Shear Strength100 MPa14500 psi ASTM D 732
Izod Impact, Notched0.4 J/cm0.749 ft-lb/in 23 C; ASTM D 256
Izod Impact, Notched (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched13 J/cm24.4 ft-lb/in 23 C; ASTM D 4812
Izod Impact, Notched, Low Temp (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.23.2 50 Hz; IEC 60250
Dielectric Strength18.6 kV/mm472 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength29 kV/mm737 kV/in in oil, 1.6 mm; IEC 60243-1
Dissipation Factor0.00150.0015 50 Hz; IEC 60250
Arc Resistance127 sec127 sec Tungsten; ASTM D 495
Comparative Tracking Index100 V100 V M; IEC 60112/3rd
Comparative Tracking Index150 V150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C45 µm/m-°C25 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C45 µm/m-°C25 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.26 W/m-K1.8 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)210 °C410 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)221 °C430 °F ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)200 °C392 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)215 °C419 °F ASTM D 648
Vicat Softening Point220 °C428 °F B/120; ISO 306
Vicat Softening Point222 °C432 °F B/50; ISO 306
UL RTI, Electrical105 °C221 °F UL 746B
UL RTI, Mechanical with Impact105 °C221 °F UL 746B
UL RTI, Mechanical without Impact105 °C221 °F UL 746B
Flammability, UL94V-0V-0 1.5 mm
Flammability Test3.23.2 mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2
NBS Smoke Density55 Flaming, Ds 4 min; ASTM E 662
Oxygen Index47 %47 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Needle Flame Test, 3.2 mm, Burn Time sPASSES IEC 60695-2-2
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。