Physical Properties | Metric | English | Comments |
|
Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
Density | 1.41 g/cc | 0.0509 lb/in³ | ASTM D 792 |
Water Absorption | 0.07 % | 0.07 % | 24 hours; ASTM D 570 |
Moisture Absorption at Equilibrium | 0.07 % | 0.07 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 0.2 % | 0.2 % | 23C; ISO 62 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 0.006 - 0.009 in/in | ASTM D 955 |
Melt Flow | 15 g/10 min | 15 g/10 min | cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133 |
Melt Flow | 18 g/10 min | 18 g/10 min | 250C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Rockwell R | 118 | 118 | ISO 2039/2 |
Hardness, H358/30 | 115 MPa | 16700 psi | ISO 2039/1 |
Tensile Strength, Ultimate | 100 MPa | 14500 psi | 5 mm/min; ISO 527 |
Elongation at Break | 3 % | 3 % | 5 mm/min; ISO 527 |
Tensile Modulus | 5.6 GPa | 812 ksi | 1 mm/min; ISO 527 |
Flexural Modulus | 5.1 GPa | 740 ksi | 2 mm/min; ISO 178 |
Flexural Strength | 145 MPa | 21000 psi | DIN 53452 |
Flexural Strength | 155 MPa | 22500 psi | 2 mm/min; ISO 178 |
Izod Impact, Notched | 0.55 J/cm | 1.03 ft-lb/in | 23 C; ASTM D 256 |
Izod Impact, Notched (ISO) | 5 kJ/m² | 2.38 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Unnotched (ISO) | 30 kJ/m² | 14.3 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | 30 kJ/m² | 14.3 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1U |
Izod Impact, Notched, Low Temp (ISO) | 4 kJ/m² | 1.9 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1A |
Izod Impact, Notched, Low Temp (ISO) | 5 kJ/m² | 2.38 ft-lb/in² | 80*10*4 -20 C; ISO 180/ 1A |
Izod Impact, Notched, Low Temp (ISO) | 5 kJ/m² | 2.38 ft-lb/in² | 80*10*4 -40 C; ISO 180/ 1A |
Charpy Impact Unnotched | 3 J/cm² | 14.3 ft-lb/in² | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.4 J/cm² | 1.9 ft-lb/in² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 3 J/cm² | 14.3 ft-lb/in² | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched | 0.5 J/cm² | 2.38 ft-lb/in² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Taber Abrasion, mg/1000 Cycles | 16 | 16 | CS-17, 1 kg; GE Test |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.9 | 2.9 | 1 MHz; IEC 60250 |
Dielectric Constant | 3 | 3 | 50 Hz; IEC 60250 |
Dielectric Strength | 18 kV/mm | 457 kV/in | in oil, 3.2 mm; IEC 60243-1 |
Dielectric Strength | 20 kV/mm | 508 kV/in | Short time, 3.2 mm; ASTM D 149 |
Dielectric Strength | 24 kV/mm | 610 kV/in | in oil, 1.6 mm; IEC 60243-1 |
Dielectric Strength | 26 kV/mm | 660 kV/in | in oil, 0.8 mm; IEC 60243-1 |
Dissipation Factor | 0.001 | 0.001 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.015 | 0.015 | 1 MHz; IEC 60250 |
Arc Resistance | 129 sec | 129 sec | Tungsten; ASTM D 495 |
Comparative Tracking Index | 250 V | 250 V | Stand. Black; IEC 60112/3rd |
Comparative Tracking Index | 275 V | 275 V | Electr Grey; IEC 60112/3rd |
Comparative Tracking Index | 300 V | 300 V | IEC 60112/3rd |
Hot Wire Ignition, HWI | 16 sec | 16 sec | UL 746A |
High Amp Arc Ignition, HAI | 112 arcs | 112 arcs | on surface; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 0.9 mm/min | 0.0354 in/min | UL 746A |
Thermal Properties |
|
CTE, linear 20°C | 35 µm/m-°C | 19.4 µin/in-°F | 23C-80C, flow; ISO 11359-2 |
CTE, linear 20°C Transverse to Flow | 95 µm/m-°C | 52.8 µin/in-°F | 23C-80C; ISO 11359-2 |
CTE, linear 100°C | 100 µm/m-°C | 55.6 µin/in-°F | 23C-150C, cross flow; ISO 11359-2 |
Thermal Conductivity | 0.19 W/m-K | 1.32 BTU-in/hr-ft²-°F | ISO 8302 |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D 648 |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 175 °C | 347 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | ASTM D 648 |
Vicat Softening Point | 200 °C | 392 °F | B/50; ISO 306 |
Vicat Softening Point | 200 °C | 392 °F | B/120; ISO 306 |
Vicat Softening Point | 210 °C | 410 °F | Rate B; ASTM D 1525 |
Vicat Softening Point | 213 °C | 415 °F | VST/A/120; DIN 53460 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
Flammability, UL94 | HB | HB | 0.75 mm |
Glow Wire Test | 750 °C | 1380 °F | Passes at 1 mm; EDF HN60S02 |
Glow Wire Test | 750 °C | 1380 °F | Passes at 1 mm; IEC 60695-2-1 |
Descriptive Properties |
|
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|
Printer friendly version |