Physical Properties | Metric | English | Comments |
|
Density | 1.3 g/cc | 0.047 lb/in³ | ASTM D 792 |
Density | 1.3 g/cc | 0.047 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 0.15 % | 0.15 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 0.45 % | 0.45 % | 23C; ISO 62 |
Linear Mold Shrinkage | 0.01 - 0.018 cm/cm | 0.01 - 0.018 in/in | Flow; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.009 - 0.018 cm/cm | 0.009 - 0.018 in/in | ASTM D 955 |
Melt Flow | 9 g/10 min | 9 g/10 min | cm3/10min; Melt Volume Rate, MVR at 250C/5.0 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, H358/30 | 87 MPa | 12600 psi | ISO 2039/1 |
Tensile Strength, Ultimate | 40 MPa | 5800 psi | 50 mm/min; ISO 527 |
Tensile Strength, Yield | 45 MPa | 6530 psi | 50 mm/min; ISO 527 |
Elongation at Break | 35 % | 35 % | 50 mm/min; ISO 527 |
Elongation at Yield | 5 % | 5 % | 50 mm/min; ISO 527 |
Tensile Modulus | 1.85 GPa | 268 ksi | 1 mm/min; ISO 527 |
Flexural Modulus | 1.8 GPa | 261 ksi | 2 mm/min; ISO 178 |
Flexural Yield Strength | 65 MPa | 9430 psi | 2 mm/min; ISO 178 |
Izod Impact, Notched (ISO) | 50 kJ/m² | 23.8 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | NB | NB | 80*10*4 -30 C; ISO 180/ 1U |
Izod Impact, Notched, Low Temp (ISO) | 20 kJ/m² | 9.52 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1A |
Izod Impact, Notched, Low Temp (ISO) | 40 kJ/m² | 19 ft-lb/in² | 80*10*4 -10 C; ISO 180/ 1A |
Charpy Impact Unnotched | NB | NB | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 1.8 J/cm² | 8.57 ft-lb/in² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | NB | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched | 5 J/cm² | 23.8 ft-lb/in² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Taber Abrasion, mg/1000 Cycles | 33 | 33 | CS-17, 1 kg; GE Test |
Electrical Properties |
|
Volume Resistivity | Min 1e+015 ohm-cm | Min 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.7 | 2.7 | 1 MHz; IEC 60250 |
Dielectric Constant | 2.8 | 2.8 | 50 Hz; IEC 60250 |
Dielectric Strength | 16 kV/mm | 406 kV/in | in oil, 3.2 mm; IEC 60243-1 |
Dissipation Factor | 0.003 | 0.003 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.013 | 0.013 | 1 MHz; IEC 60250 |
Comparative Tracking Index | 225 V | 225 V | IEC 60112/3rd |
Thermal Properties |
|
CTE, linear 20°C | 105 µm/m-°C | 58.3 µin/in-°F | 23C-60C, flow; ISO 11359-2 |
CTE, linear 20°C Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | 23C-60C; ISO 11359-2 |
Deflection Temperature at 0.46 MPa (66 psi) | 120 °C | 248 °F | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 80 °C | 176 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Vicat Softening Point | 130 °C | 266 °F | B/50; ISO 306 |
Vicat Softening Point | 135 °C | 275 °F | B/120; ISO 306 |
Vicat Softening Point | 165 °C | 329 °F | A/50; ISO 306 |
Flammability, UL94 | V-2 | V-2 | 1.6 mm; UL 94 by GE |
Flammability, UL94 | V-1 | V-1 | 2 mm; UL 94 by GE |
Flammability, UL94 | V-0 | V-0 | 4 mm; UL 94 by GE |
Oxygen Index | 25 % | 25 % | ISO 4589 |
Glow Wire Test | 850 °C | 1560 °F | Passes at 2.5 mm; IEC 60695-2-1 |
Glow Wire Test | 960 °C | 1760 °F | Passes at 3.2 mm; IEC 60695-2-1 |
Descriptive Properties |
|
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|
Printer friendly version |