Physical Properties | Metric | English | Comments |
|
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D 792 |
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 0.08 % | 0.08 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 0.34 % | 0.34 % | 23C; ISO 62 |
Viscosity | 750000 cP | 750000 cP | Melt Viscosity; GE Test |
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | Flow; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.009 - 0.018 cm/cm | 0.009 - 0.018 in/in | ASTM D 955 |
Melt Flow | 6 g/10 min | 6 g/10 min | cm3/10min; Melt Volume Rate, MVR at 250C/1.2 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Rockwell R | 117 | 117 | ISO 2039/2 |
Hardness, H358/30 | 110 MPa | 16000 psi | ISO 2039/1 |
Tensile Strength, Ultimate | 30 MPa | 4350 psi | 50 mm/min; ISO 527 |
Tensile Strength, Yield | 51 MPa | 7400 psi | ASTM D 638 |
Tensile Strength, Yield | 55 MPa | 7980 psi | 50 mm/min; ISO 527 |
Elongation at Break | 100 % | 100 % | 50 mm/min; ISO 527 |
Elongation at Break | 300 % | 300 % | ASTM D 638 |
Elongation at Yield | 3.5 % | 3.5 % | 50 mm/min; ISO 527 |
Tensile Modulus | 2.4 GPa | 348 ksi | 1 mm/min; ISO 527 |
Flexural Modulus | 2.3 GPa | 334 ksi | 2 mm/min; ISO 178 |
Flexural Modulus | 2.34 GPa | 339 ksi | DIN 53457 |
Flexural Yield Strength | 75 MPa | 10900 psi | 2 mm/min; ISO 178 |
Flexural Yield Strength | 82 MPa | 11900 psi | DIN 53452 |
Ultimate Compressive Strength | 89 MPa | 12900 psi | ASTM D 695 |
Shear Strength | 53 MPa | 7690 psi | ASTM D 732 |
Izod Impact, Notched | 0.53 J/cm | 0.993 ft-lb/in | 23 C; ASTM D 256 |
Izod Impact, Notched (ISO) | 6 kJ/m² | 2.86 ft-lb/in² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Unnotched | 16 J/cm | 30 ft-lb/in | 23 C; ASTM D 4812 |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | NB | NB | 80*10*4 -30 C; ISO 180/ 1U |
Izod Impact, Notched, Low Temp (ISO) | 5 kJ/m² | 2.38 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1A |
Charpy Impact Unnotched | NB | NB | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.4 J/cm² | 1.9 ft-lb/in² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | NB | NB | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched | 0.55 J/cm² | 2.62 ft-lb/in² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Electrical Properties |
|
Volume Resistivity | Min 1e+015 ohm-cm | Min 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.4 | 2.4 | 1 MHz; IEC 60250 |
Dielectric Constant | 2.9 | 2.9 | 50 Hz; IEC 60250 |
Dielectric Constant | 3.3 | 3.3 | 100 Hz; IEC 60250 |
Dielectric Strength | 15 kV/mm | 381 kV/in | in oil, 3.2 mm; IEC 60243-1 |
Dielectric Strength | 24 kV/mm | 610 kV/in | in oil, 1.6 mm; IEC 60243-1 |
Dielectric Strength | 29 kV/mm | 737 kV/in | in oil, 0.8 mm; IEC 60243-1 |
Dissipation Factor | 0.0003 | 0.0003 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.002 | 0.002 | 100 Hz; IEC 60250 |
Dissipation Factor | 0.02 | 0.02 | 1 MHz; IEC 60250 |
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112/3rd |
Comparative Tracking Index | 600 V | 600 V | IEC 60112/3rd |
Comparative Tracking Index | 600 V | 600 V | Stand. Black; IEC 60112/3rd |
Comparative Tracking Index | 600 V | 600 V | Electr Grey; IEC 60112/3rd |
Thermal Properties |
|
CTE, linear 20°C | 120 µm/m-°C | 66.7 µin/in-°F | 23C-80C, flow; ISO 11359-2 |
CTE, linear 20°C Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | 23C-80C; ISO 11359-2 |
Deflection Temperature at 0.46 MPa (66 psi) | 120 °C | 248 °F | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 309 °F | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 54 °C | 129 °F | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 55 °C | 131 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Vicat Softening Point | 170 °C | 338 °F | B/50; ISO 306 |
Vicat Softening Point | 170 °C | 338 °F | B/120; ISO 306 |
Vicat Softening Point | 220 °C | 428 °F | A/50; ISO 306 |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | HB | HB | 1.6 mm; UL 94 by GE |
Oxygen Index | 21 % | 21 % | ISO 4589 |
Glow Wire Test | 850 °C | 1560 °F | Passes at 1 mm; IEC 60695-2-1 |
Glow Wire Test | 960 °C | 1760 °F | Passes at 3.2 mm; EDF HN60S02 |
Glow Wire Test | 960 °C | 1760 °F | Passes at 2.02 mm; IEC 60695-2-1 |
Descriptive Properties |
|
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|