SABIC Innovative Plastics VALOX 457 PBT (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesMetricEnglishComments
Density1.43 g/cc0.0517 lb/in³ ASTM D 792
Density1.43 g/cc0.0517 lb/in³ ISO 1183
Water Absorption0.06 %0.06 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.06 %0.06 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.28 %0.28 % 23C; ISO 62
Linear Mold Shrinkage0.01 - 0.014 cm/cm0.01 - 0.014 in/in Flow, 3.2 mm; ASTM D 955
Linear Mold Shrinkage0.01 - 0.014 cm/cm0.01 - 0.014 in/in Flow; ASTM D 955
Linear Mold Shrinkage, Transverse0.013 - 0.017 cm/cm0.013 - 0.017 in/in ASTM D 955
Melt Flow11 g/10 min11 g/10 min cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell R121121 ISO 2039/2
Tensile Strength, Ultimate75 MPa10900 psi 5 mm/min; ISO 527
Tensile Strength, Ultimate79 MPa11500 psi ASTM D 638
Elongation at Break3 %3 % 5 mm/min; ISO 527
Tensile Modulus3.6 GPa522 ksi 1 mm/min; ISO 527
Flexural Modulus3.5 GPa508 ksi 2 mm/min; ISO 178
Flexural Modulus3.51 GPa509 ksi DIN 53457
Flexural Strength110 MPa16000 psi 2 mm/min; ISO 178
Flexural Strength124 MPa18000 psi DIN 53452
Ultimate Compressive Strength95 MPa13800 psi ASTM D 695
Shear Strength58 MPa8410 psi ASTM D 732
Izod Impact, Notched0.32 J/cm0.599 ft-lb/in 23 C; ASTM D 256
Izod Impact, Notched (ISO)6 kJ/m²2.86 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched2.67 J/cm5 ft-lb/in 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)25 kJ/m²11.9 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)25 kJ/m²11.9 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact Unnotched3 J/cm²14.3 ft-lb/in² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.6 J/cm²2.86 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Unnotched Low Temp3 J/cm²14.3 ft-lb/in² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched0.7 J/cm²3.33 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant33 50 Hz; IEC 60250
Dielectric Constant33 1 MHz; IEC 60250
Dielectric Constant3.53.5 100 Hz; IEC 60250
Dielectric Strength15 kV/mm381 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength22 kV/mm559 kV/in Short time, 3.2 mm; ASTM D 149
Dielectric Strength23 kV/mm584 kV/in in oil, 1.6 mm; IEC 60243-1
Dielectric Strength29 kV/mm737 kV/in in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.0020.002 50 Hz; IEC 60250
Dissipation Factor0.0020.002 100 Hz; IEC 60250
Dissipation Factor0.020.02 1 MHz; IEC 60250
Arc Resistance28 sec28 sec Tungsten; ASTM D 495
Comparative Tracking Index150 V150 V Stand. Black; IEC 60112/3rd
Comparative Tracking Index175 V175 V IEC 60112/3rd
Comparative Tracking Index225 V225 V Electr Grey; IEC 60112/3rd
Hot Wire Ignition, HWI20 sec20 sec UL 746A
High Amp Arc Ignition, HAI19 arcs19 arcs on surface; UL 746A
High Voltage Arc-Tracking Rate, HVTR21 mm/min0.827 in/min UL 746A

Thermal Properties
CTE, linear 20°C80 µm/m-°C44.4 µin/in-°F 23C-80C, flow; ISO 11359-2
CTE, linear 20°C Transverse to Flow100 µm/m-°C55.6 µin/in-°F 23C-80C; ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)200 °C392 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)204 °C399 °F ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)140 °C284 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)151 °C304 °F ASTM D 648
Vicat Softening Point190 °C374 °F B/50; ISO 306
Vicat Softening Point210 °C410 °F B/120; ISO 306
Vicat Softening Point222 °C432 °F Rate B; ASTM D 1525
UL RTI, Electrical120 °C248 °F UL 746B
UL RTI, Mechanical with Impact120 °C248 °F UL 746B
UL RTI, Mechanical without Impact140 °C284 °F UL 746B
Flammability, UL94V-0V-0 0.71 mm
Flammability, UL9477 94-3 mm
Flammability Test11 mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2
Oxygen Index30 %30 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 1 mm; EDF HN60S02
Glow Wire Test960 °C1760 °F Passes at 1 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。