SABIC Innovative Plastics VALOX 508 PBT (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesMetricEnglishComments
Density1.5 g/cc0.0542 lb/in³ ASTM D 792
Density1.5 g/cc0.0542 lb/in³ ISO 1183
Water Absorption0.06 %0.06 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.06 %0.06 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.09 %0.09 % 23C; ISO 62
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.009 cm/cm0.005 - 0.009 in/in ASTM D 955
Melt Flow8 g/10 min8 g/10 min cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell R119119 ISO 2039/2
Hardness, H358/30122 MPa17700 psi ISO 2039/1
Tensile Strength, Ultimate110 MPa16000 psi ASTM D 638
Tensile Strength, Ultimate115 MPa16700 psi 5 mm/min; ISO 527
Elongation at Break2 %2 % 5 mm/min; ISO 527
Elongation at Break3 %3 % ASTM D 638
Tensile Modulus9 GPa1310 ksi 1 mm/min; ISO 527
Flexural Modulus6.9 GPa1000 ksi DIN 53457
Flexural Modulus8 GPa1160 ksi 2 mm/min; ISO 178
Flexural Strength170 MPa24700 psi DIN 53452
Flexural Strength170 MPa24700 psi 2 mm/min; ISO 178
Ultimate Compressive Strength115 MPa16700 psi ASTM D 695
Shear Strength56 MPa8120 psi ASTM D 732
Izod Impact, Notched1.05 J/cm1.97 ft-lb/in 23 C; ASTM D 256
Izod Impact, Notched (ISO)8 kJ/m²3.81 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)45 kJ/m²21.4 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)40 kJ/m²19 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)7 kJ/m²3.33 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact Unnotched4.5 J/cm²21.4 ft-lb/in² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.65 J/cm²3.09 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Unnotched Low Temp4.5 J/cm²21.4 ft-lb/in² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched0.75 J/cm²3.57 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles5050 CS-17, 1 kg; GE Test

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.23.2 1 MHz; IEC 60250
Dielectric Constant3.33.3 50 Hz; IEC 60250
Dielectric Constant3.63.6 100 Hz; IEC 60250
Dielectric Strength16 kV/mm406 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength23 kV/mm584 kV/in in oil, 1.6 mm; IEC 60243-1
Dielectric Strength24 kV/mm610 kV/in Short time, 3.2 mm; ASTM D 149
Dielectric Strength24 kV/mm610 kV/in Short time, 1.0 mm; IEC 60243-1
Dielectric Strength30 kV/mm762 kV/in in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.0010.001 50 Hz; IEC 60250
Dissipation Factor0.00140.0014 100 Hz; IEC 60250
Dissipation Factor0.0130.013 1 MHz; IEC 60250
Arc Resistance62 sec62 sec Tungsten; ASTM D 495
Comparative Tracking Index150 V150 V M; IEC 60112/3rd
Comparative Tracking Index250 V250 V IEC 60112/3rd
Comparative Tracking Index250 V250 V Stand. Black; IEC 60112/3rd
Comparative Tracking Index275 V275 V Electr Grey; IEC 60112/3rd
Hot Wire Ignition, HWI66 sec66 sec UL 746A
High Amp Arc Ignition, HAI15 arcs15 arcs on surface; UL 746A
High Voltage Arc-Tracking Rate, HVTR1.8 mm/min0.0709 in/min UL 746A

Thermal Properties
CTE, linear 20°C25 µm/m-°C13.9 µin/in-°F 23C-80C, flow; ISO 11359-2
CTE, linear 20°C Transverse to Flow100 µm/m-°C55.6 µin/in-°F 23C-80C; ISO 11359-2
CTE, linear 100°C105 µm/m-°C58.3 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)206 °C403 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)215 °C419 °F ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)160 °C320 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)175 °C347 °F ASTM D 648
Vicat Softening Point170 °C338 °F B/50; ISO 306
Vicat Softening Point175 °C347 °F B/120; ISO 306
Vicat Softening Point215 °C419 °F Rate B; ASTM D 1525
Vicat Softening Point217 °C423 °F A/50; ISO 306
UL RTI, Electrical125 °C257 °F UL 746B
UL RTI, Mechanical with Impact110 °C230 °F UL 746B
UL RTI, Mechanical without Impact125 °C257 °F UL 746B
Flammability, UL94HBHB 1.5 mm
Oxygen Index21 %21 % ISO 4589
Glow Wire Test750 °C1380 °F Passes at 1 mm; EDF HN60S02
Glow Wire Test750 °C1380 °F Passes at 1 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。