SABIC Innovative Plastics LEXAN® 4701 Polyphthalate Carbonate, Unfilled, Injection Grade
Subcategory: Polycarbonate; Polymer; Polyphthalate Carbonate; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
Physical Properties | Metric | English | Comments |
|
Density | 1.2 g/cc | 0.0434 lb/in³ | ASTM D792 |
Water Absorption | 0.19 % | 0.19 % | 24 hrs; 20°C; ASTM D570 |
Linear Mold Shrinkage | 0.008 - 0.01 cm/cm | 0.008 - 0.01 in/in | 3.2 mm sample |
Melt Flow | 2 g/10 min | 2 g/10 min | 300°C/1.2kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 78 MPa | 11300 psi | ASTM D638 |
Elongation at Break | 78 % | 78 % | ASTM D638 |
Flexural Modulus | 2.3 GPa | 334 ksi | 3.2 mm sample; ASTM D790 |
Flexural Yield Strength | 97 MPa | 14100 psi | ASTM D790 |
Izod Impact, Notched | 3.7 J/cm | 6.93 ft-lb/in | 3.2 mm sample; ASTM D256 |
Electrical Properties |
|
Electrical Resistivity | 2e+017 ohm-cm | 2e+017 ohm-cm | ASTM D257 |
Dielectric Constant | 3.1 | 3.1 | 1 MHz; ASTM D150 |
Dielectric Constant, Low Frequency | 3.27 | 3.27 | 60 Hz; ASTM D150 |
Dissipation Factor, Low Frequency | 0.0016 | 0.0016 | 60 Hz; ASTM D150 |
Thermal Properties |
|
CTE, linear 20°C | 81 µm/m-°C | 45 µin/in-°F | ASTM E831 |
Deflection Temperature at 1.8 MPa (264 psi) | 148 °C | 298 °F | 3.2 mm (1/8 in.) sample; ASTM D648 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical without Impact | 130 °C | 266 °F | UL 746B |
Flammability, UL94 | HB | HB | 1.6 mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|