SABIC Innovative Plastics LEXAN® SP6400R Polycarbonate, Unfilled, Injection Grade
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
Physical Properties | Metric | English | Comments |
|
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | 3.2 mm sample |
Melt Flow | 28 g/10 min | 28 g/10 min | 300°C/1.2kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 55 MPa | 7980 psi | ASTM D638 |
Elongation at Break | 100 % | 100 % | ASTM D638 |
Flexural Modulus | 2.1 GPa | 305 ksi | 3.2 mm sample; ASTM D790 |
Flexural Yield Strength | 79 MPa | 11500 psi | ASTM D790 |
Izod Impact, Notched | 6.9 J/cm | 12.9 ft-lb/in | 3.2 mm sample; ASTM D256 |
Izod Impact, Notched, Low Temp | 6.4 J/cm | 12 ft-lb/in | -40°C; 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 95 °C | 203 °F | 3.2 mm (1/8 in.) sample; ASTM D648 |
Processing Properties |
|
Processing Temperature | 248 - 271 °C | 478 - 520 °F | Suggested injection molding melt temperature |
Mold Temperature | 48 - 82 °C | 118 - 180 °F | |
Drying Temperature | 107 °C | 225 °F | |
Dry Time | 3 - 4 hour | 3 - 4 hour | 24 hr Max |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|