SABIC Innovative Plastics ULTEM® HTX1050F Polyetherimide, Unfilled, Injection/Extrusion Grade

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.26 g/cc0.0455 lb/in³ ASTM D792
Melt Flow8 g/10 min8 g/10 min 335°C/6.6kg; ASTM D1238

Mechanical Properties
Tensile Strength, Ultimate91 MPa13200 psi ASTM D638
Elongation at Break60 %60 % ASTM D638
Flexural Modulus2.8 GPa406 ksi 6.4 mm sample; ASTM D790
Flexural Yield Strength134 MPa19400 psi ASTM D790
Izod Impact, Notched1.9 J/cm3.56 ft-lb/in 3.2 mm sample; ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)200 °C392 °F 6.4 mm (0.25 in.) sample; ASTM D648

Processing Properties
Processing Temperature348 - 371 °C658 - 700 °F Suggested injection molding melt temperature
Mold Temperature135 - 162 °C275 - 324 °F 
Drying Temperature135 °C275 °F 
Dry Time4 - 6 hour4 - 6 hour 10 hr Max.
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。