SABIC Innovative Plastics ULTEM® 7642 PEI, Unfilled
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 152 MPa | 22000 psi | ASTM D638 |
Elongation at Break | 2 % | 2 % | ASTM D638 |
Flexural Modulus | 8.957 GPa | 1300 ksi | ASTM D790 |
Izod Impact, Notched | 0.53 J/cm | 0.993 ft-lb/in | 23°C (73.4°F) |
Electrical Properties |
|
Surface Resistance | 1e+007 ohm | 1e+007 ohm | |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 354 - 376 °C | 669 - 709 °F | melt temperature |
Mold Temperature | 135 - 162 °C | 275 - 324 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|