Gharda Chemicals GAFONE™ 3200 PES, High Viscosity Grade
Subcategory: Filled/Reinforced Thermoplastic; Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes: High viscosity grade for membrane and coating applications. Characteristics: - Very high rigidity
- Good dielectric properties
- High mechanical strength
- Good dimensional stability
- Good resistance to hydrolysis and sterilization
- Good oxidative stability
- Inherent flame retardance
Applications: - Reusable hypodermic syringes
- Surgical instruments and components
- Printed circuit boards
- Circuit breaker components
- Oil level indicators
- Heat exchanger parts
- Engine components
- Household appliances
- Filter housings
- Sanitary and pipe fittings
Information provided by Gharda.
Physical Properties | Metric | English | Comments |
|
Melt Flow | 20 - 25 g/10 min | 20 - 25 g/10 min | 380°C, 2.16 kg, 6 mins; ASTM D1238 |
Thermal Properties |
|
Maximum Service Temperature, Air | 210 °C | 410 °F | Temperature resistance |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|