SABIC Innovative Plastics Lexan® 9600 Polycarbonate Sheet
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Lexan® 9600 sheet offers improved flammability characteristics than conventional LEXAN polycarbonate sheet. It is formulated to meet the standards of UL Bulletin, Class I. Developed to meet industry flammability codes, LEXAN 9600 sheet is widely used in power tools, electrical appliances, safety equipment and aircraft components. The improved flammability and slightly higher heat deflection temperature of LEXAN 9600 sheet are accompanied by essentially the same physical, electrical, chemical and fabricating properties exhibited by standard LEXAN Sheet. Information provided by Aurora Technologies.
Physical Properties | Metric | English | Comments |
|
Water Absorption | 0.2 % | 0.2 % | |
Mechanical Properties |
|
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | |
Tensile Strength, Yield | 65.5 MPa | 9500 psi | |
Elongation at Break | 95 % | 95 % | |
Flexural Modulus | 2.55 GPa | 370 ksi | |
Flexural Strength | 93.1 MPa | 13500 psi | |
Compressive Strength | 86.2 MPa | 12500 psi | |
Izod Impact, Unnotched | NB | NB | |
Izod Impact, Notched | 6.41 - 8.54 J/cm | 12 - 16 ft-lb/in | Edgewise |
Izod Impact, Notched | 1.28 J/cm | 2.4 ft-lb/in | |
Thermal Properties |
|
CTE, linear 68°F | 67.5 µm/m-°C | 37.5 µin/in-°F | |
Maximum Service Temperature, Air | 138 °C | 280 °F | Deflection Temp; Load not specified |
Flammability, UL94 | V-0 | V-0 | |
Optical Properties |
|
Transmission, Visible | 85 % | 85 % | 1/8 in disk |
Descriptive Properties | |
Color | Clear | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|