EMS-Grivory Grilon PVS-3H Nylon 6, 30% glass fiber reinforced, As Conditioned
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 6; Polymer; Thermoplastic
Key Words: Polyamide 6
Material Notes: Data provided by EMS-Grivory. Normal viscosity, heat stabilized PA6 molding type with 30% glass fibers. Easy flowing, very good processing, for articles demanding an excellent surface finish. Applications: Stiff molding components with high demand for a good finish, insulators, high and low voltage components, power tool housings, seat levers, car electrics and electronics.
Physical Properties | Metric | English | Comments |
|
Density | 1.35 g/cc | 0.0488 lb/in³ | |
Water Absorption | 7 % | 7 % | |
Moisture Absorption at Equilibrium | 2 % | 2 % | Humidity Absorption |
Viscosity Test | 145 cm³/g | 145 cm³/g | Viscosity Number |
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | Parallel |
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Melt Flow | 70 g/10 min | 70 g/10 min | 275°C/5kg |
Mechanical Properties |
|
Tensile Strength, Yield | 125 MPa | 18100 psi | |
Elongation at Break | 8 % | 8 % | |
Elongation at Yield | 5 % | 5 % | |
Tensile Modulus | 6 GPa | 870 ksi | |
Charpy Impact Unnotched | 9 J/cm² | 42.8 ft-lb/in² | |
Charpy Impact, Notched, Low Temp | 0.9 J/cm² | 4.28 ft-lb/in² | |
Charpy Impact, Unnotched Low Temp | 7 J/cm² | 33.3 ft-lb/in² | |
Charpy Impact, Notched | 2 J/cm² | 9.52 ft-lb/in² | |
Tensile Creep Modulus, 1 hour | 7000 MPa | 1.02e+006 psi | |
Tensile Creep Modulus, 1000 hours | 5000 MPa | 725000 psi | |
Electrical Properties |
|
Electrical Resistivity | 1e+013 ohm-cm | 1e+013 ohm-cm | |
Surface Resistance | 1e+012 ohm | 1e+012 ohm | |
Dielectric Constant | 5 | 5 | 1 MHz |
Dielectric Constant, Low Frequency | 7 | 7 | 100 Hz |
Dielectric Strength | 37 kV/mm | 940 kV/in | |
Dissipation Factor | 0.09 | 0.09 | 1 MHz |
Dissipation Factor, Low Frequency | 0.1 | 0.1 | 100 Hz |
Comparative Tracking Index | 500 V | 500 V | |
Thermal Properties |
|
CTE, linear 20°C | 20 µm/m-°C | 11.1 µin/in-°F | Parallel to flow |
CTE, linear 20°C Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | |
Melting Point | 222 °C | 432 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | |
Vicat Softening Point | 212 °C | 414 °F | |
Flammability, UL94 | HB | HB | 1.6 mm nominal thickness |
Oxygen Index | 21.5 % | 21.5 % | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|