EMS-Grivory Grilon® RVZ-15H.1 Nylon 6, 15% Glass Fiber Filled, Dry As Molded
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 6; Polymer; Thermoplastic
Material Notes: Grilon RVZ-15H.1 Black 9697 is an extrusion blow moldable, 15% glass fiber reinforced, high viscosity, heat stabilized polyamide 6 that exhibits high impact strength even at low temperatures. Due to its very high melt strength, Grilon RVZ-15H.1 is particularly well suited for the production of large extrusion blow molded articles. It can easily be processed on conventional and 3D machines. Grilon RVZ-15H.1 is suitable for technical articles of all kinds, especially automotive applications. Examples of possible applications include; Air ducts for turbo-chargers, Oil filler pipes, Air ducts, Fuel and oil containers and Resonators. Information provided by EMS-Grivory
| Physical Properties | Metric | English | Comments |
|
| Density | 1.19 g/cc | 0.043 lb/in³ | ASTM D792 |
| Water Absorption | 1.23 % | 1.23 % | 24 hr immersion; ASTM D570 |
| Water Absorption | 2.5 % | 2.5 % | 23°C / 50% RH; ASTM D570 |
| Water Absorption at Saturation | 8 % | 8 % | 23°C in water; ASTM D570 |
| Linear Mold Shrinkage | 0.003 cm/cm | 0.003 in/in | ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.007 cm/cm | 0.007 in/in | ASTM D955 |
Mechanical Properties |
|
| Hardness, Shore D | 85 | 85 | |
| Tensile Strength at Break | 90 MPa | 13100 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Flexural Modulus | 3.565 GPa | 517 ksi | ASTM D790 |
| Flexural Strength | 133 MPa | 19300 psi | ASTM D790 |
| Izod Impact, Notched | 2.11 J/cm | 3.95 ft-lb/in | ASTM D256 |
Thermal Properties |
|
| CTE, linear 20°C | 120 µm/m-°C | 66.7 µin/in-°F | transverse; ASTM E831 |
| CTE, linear 20°C | 35 µm/m-°C | 19.4 µin/in-°F | longitudinal; ASTM E831 |
| Melting Point | 221 °C | 430 °F | DSC |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 181 °C | 358 °F | ASTM D648 |
Processing Properties |
|
| Feed Temperature | 100 - 160 °C | 212 - 320 °F | Extrusion |
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 3 (Extrusion) |
| Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 (Extrusion) |
| Front Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 1 (Extrusion) |
| Adapter Temperature | 240 - 250 °C | 464 - 482 °F | Extrusion |
| Die Temperature | 230 - 250 °C | 446 - 482 °F | Extrusion |
| Melt Temperature | 250 - 260 °C | 482 - 500 °F | Extrusion |
| Mold Temperature | 40 - 90 °C | 104 - 194 °F | Extrusion |
| Drying Temperature | 100 °C | 212 °F | Vacuum Oven |
| Drying Temperature | 80 °C | 176 °F | Dehumidifying Dryer (dew point at -40°F) |
| Drying Temperature | 80 °C | 176 °F | Circulating Air Oven |
| Dry Time | 4 - 16 hour | 4 - 16 hour | Vacuum Oven |
| Dry Time | 4 - 16 hour | 4 - 16 hour | Dehumidifying Dryer (dew point at -40°F) |
| Dry Time | 6 - 16 hour | 6 - 16 hour | Circulating Air Oven |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|