EMS-Grivory Grilon® XS 1306.1 Nylon 610, Dry As Molded
Subcategory: Nylon; Nylon 610; Polymer; Thermoplastic
Material Notes: Grilon XS 1306.1 is a medium viscosity, nylon 6.10 homopolymer. It is particularly well-suited for monofilaments. Grilon XS 1306.1 exhibits excellent strength, toughness, ductility, heat stability and abrasion resistance. Grilon XS 1306.1 also offers very good resistance to a wide range of chemicals, solvents, oils and greases.Information provided by EMS-Grivory
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.08 g/cc | 0.039 lb/in³ | ASTM D792 |
| Water Absorption | 0.46 % | 0.46 % | 24 hr immersion; ASTM D570 |
Mechanical Properties |
|
| Hardness, Shore D | 81 | 81 | |
| Tensile Strength at Break | 61 MPa | 8850 psi | ASTM D638 |
| Elongation at Break | 30 % | 30 % | ASTM D638 |
| Flexural Modulus | 2.145 GPa | 311 ksi | ASTM D790 |
| Flexural Strength | 90 MPa | 13100 psi | ASTM D790 |
| Izod Impact, Notched | 0.427 J/cm | 0.8 ft-lb/in | ASTM D256 |
Thermal Properties |
|
| Melting Point | 222 °C | 432 °F | DSC |
| Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | 277 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 53 °C | 127 °F | ASTM D648 |
Processing Properties |
|
| Rear Barrel Temperature | 232 °C | 450 °F | Extrusion |
| Rear Barrel Temperature | 245 °C | 473 °F | Injection Molding |
| Middle Barrel Temperature | 232 °C | 450 °F | Extrusion |
| Middle Barrel Temperature | 255 °C | 491 °F | Injection Molding |
| Front Barrel Temperature | 227 °C | 441 °F | Extrusion |
| Front Barrel Temperature | 265 °C | 509 °F | Injection Molding |
| Nozzle Temperature | 255 °C | 491 °F | Injection Molding |
| Die Temperature | 232 °C | 450 °F | Extrusion |
| Melt Temperature | 233 °C | 451 °F | Extrusion |
| Melt Temperature | 265 °C | 509 °F | Injection Molding |
| Mold Temperature | 60 °C | 140 °F | Injection Molding |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.

|