| Physical Properties | Metric | English | Comments |
|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
| Water Absorption | 1.5 % | 1.5 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 3.5 % | 3.5 % | ISO 62 |
| Water Vapor Transmission | 10 g/m²/day | 0.644 g/100 in²/day | 23°C / 85% RH; DIS/ISO 15106-1 |
| Oxygen Transmission | 10.1 cc-mm/m²-24hr-atm | 25.7 cc-mil/100 in²-24hr-atm | 23°C / 85% RH; DIS/ISO 15105-1 |
| Oxygen Transmission | 15.2 cc-mm/m²-24hr-atm | 38.6 cc-mil/100 in²-24hr-atm | 23°C / 0% RH; DIS/ISO 15105-1 |
| Carbon Dioxide Transmission | 60.8 cc-mm/m²-24hr-atm | 154 cc-mil/100 in²-24hr-atm | 23°C / 0% RH; DIS/ISO 15105-2 |
| Carbon Dioxide Transmission | 60.8 cc-mm/m²-24hr-atm | 154 cc-mil/100 in²-24hr-atm | 23°C / 85% RH; DIS/ISO 15105-2 |
| Melt Flow | 163 g/10 min | 163 g/10 min | 275°C / 5kg; ISO 1133 |
Mechanical Properties |
|
| Tensile Strength at Break | 70 MPa | 10200 psi | normal; ISO 527-3 |
| Film Tensile Strength at Yield, MD | 33 MPa | 4790 psi | ISO 527-3 |
| Film Tensile Strength at Break, MD | 75 MPa | 10900 psi | ISO 527-3 |
| Film Elongation at Break, MD | 800 % | 800 % | ISO 527-3 |
| Film Elongation at Yield, MD | 8 % | 8 % | ISO 527-3 |
| Tensile Strength, Yield | 30 MPa | 4350 psi | normal; ISO 527-3 |
| Elongation at Break | 800 % | 800 % | normal; ISO 527-3 |
| Elongation at Yield | 7 % | 7 % | normal; ISO 527-3 |
| Tensile Modulus | 0.8 GPa | 116 ksi | 4 mm bar; ISO 527-2 |
| Tear Strength Test | 50 | 50 | [N/mm]; ISO 6383-1 |
Thermal Properties |
|
| Melting Point | 178 °C | 352 °F | ISO 11357 |
Optical Properties |
|
| Gloss | 60 % | 60 % | 60°; ISO 2813 |
|
Printer friendly version |