MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

EMS-Grivory Grilon® XS 1423 Natural Nylon 6, Dry As Molded

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Nylon; Nylon 6; Polymer; Thermoplastic

Material Notes:
Grilon XS1423 Natural is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade.

Grilon XS1423 Natural is used typically for co-extruded fuel lines, coolant pipes in deep freezer units, vulcanization mandrels, and vacuum lines.

Information provided by EMS-Grivory

Physical PropertiesMetricEnglishComments
Density1.08 g/cc0.039 lb/in³ ASTM D792
Melt Flow18.4 g/10 min18.4 g/10 min 275°C / 5kg; ASTM D1238

Mechanical Properties
Tensile Strength at Break54.3 MPa7880 psi 50 mm/min; ASTM D638
Elongation at Break41 %41 % 50 mm/min; ASTM D638
Flexural Modulus0.348 GPa50.5 ksi 2 mm/min; ASTM D790

Processing Properties
Processing Temperature230 - 260 °C446 - 500 °F Compression zone
Processing Temperature230 - 260 °C446 - 500 °F Metering zone
Feed Temperature190 - 250 °C374 - 482 °F 
Nozzle Temperature230 - 260 °C446 - 500 °F 
Melt Temperature230 - 260 °C446 - 500 °F Basic Machine Settings
Head Temperature230 - 260 °C446 - 500 °F 
Drying TemperatureMax 80 °CMax 176 °F Desiccant Dryer (dew point at -30°C)
Drying TemperatureMax 100 °CMax 212 °F Vacuum Oven
Dry Time4 - 12 hour4 - 12 hour Desiccant Dryer (dew point at -30°C)
Dry Time4 - 12 hour4 - 12 hour Vacuum Oven
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。