PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.Description/Features: - PEI (Polyetherimide)
- 5% Carbon Fiber Reinforced
- ESD Protection
- Antistatic
- Static Dissipative
Applications: - EMI?RFI Shielding
- Printer Components
- Enclosures
- Fuel Systems
Processing Method: Injection Molding Information provided by PolyOne Corporation
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 |
Water Absorption | 0.25 % | 0.25 % | 24 hr. Immersion, 0.125 in; ASTM D570 |
Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | ASTM D955 |
Mechanical Properties |
|
Tensile Strength @ Yield | 124 MPa | 18000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
Elongation at Break | 4 - 5 % | 4 - 5 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 4.48 GPa | 650 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Flexural Strength | 193 MPa | 28000 psi | ASTM D790 |
Izod Impact, Notched | 0.481 J/cm | 0.9 ft-lb/in | Method A, Injection Molded, 0.250 in bars, 73°F(23°C); ASTM D256 |
Electrical Properties |
|
Volume Resistivity | 1000 - 100000 ohm-cm | 1000 - 100000 ohm-cm | ASTM D257 |
Surface Resistivity per Square | 1000 - 100000 ohm | 1000 - 100000 ohm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 207 °C | 405 °F | Unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 199 °C | 390 °F | Unannealed; ASTM D648 |
Processing Properties |
|
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|