PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Description/Features: - PEI (Polyetherimide)
- Unfilled
- Hi-Temp
Applications: Multi-purpose Processing Method: Injection Molding Information provided by PolyOne Corporation
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
| Water Absorption | 0.25 % | 0.25 % | 24 hr. Immersion, 0.125 in; ASTM D570 |
| Linear Mold Shrinkage | 0.007 - 0.009 cm/cm | 0.007 - 0.009 in/in | ASTM D955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 105 MPa | 15200 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
| Elongation at Break | 7 - 8 % | 7 - 8 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 2.96 GPa | 430 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 2.9 GPa | 420 ksi | ASTM D790 |
| Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F(23°C); ASTM D256 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | Unannealed; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 327 - 371 °C | 620 - 700 °F | Molding |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|