PolyOne Geon® 121A Polyvinyl Chloride Homopolymer (PVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Good multi-purpose resin for a wide range of end uses
- High molecular weight resin providing good fused film physical properties
- Good chemical foamability for producing medium to high density foams
- Good dispersability for easier plastisol preparation
Applications: - Recommended for med-high density foam or solid apps. where good fused film properties are required
- Spread Coating
- Spray Coating
- Dip Coating and Molding
- Slush and Rotational Molding
Dispersion Polymerization ProcessDisclaimer: Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent "typical" values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Note: The values set forth represent "typical" values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Manufacturing Location: This resin is produced at PolyOne's Pedricktown, NJ facility, which is ISO 9002 certified. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Information provided by PolyOne Corporation.
We're sorry, but our sources do not report any other information for this material. We are limited by the information available from our sources, which often are not as complete as we would like. Sometimes you will see this message during a MatWeb internal update, especially around 07:00 GMT Sundays.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|