PolyOne Geon® 1351 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Enhanced Heat Stability
- High Flow
Applications: - General Purpose
- Fence Wire Coating
Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 63 | 63 | 15 sec; ASTM D2240 |
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | 20 in/min, 100% in/in; ASTM D638 |
Tensile Strength, Ultimate | 21.7 MPa | 3150 psi | 20 in/min; ASTM D638 |
Elongation at Break | 170 % | 170 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | 0 °C | 32 °F | ASTM D746 |
Processing Properties |
|
Melt Temperature | 174 - 179 °C | 345 - 355 °F | Extrusion |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|