PolyOne Geon® 2121C Vinyl Compound - Rigid (RPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

A Clear Rigid PVC Compound designed specifically for water bottle applications.

Description/Features:

  • Transparent
  • High Impact
  • High Gloss

Applications:

  • FDA (Food Contact)
  • Bottles

Market:

  • Packaging

Processing Method:

  • Blow Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Density0.801 g/cc0.0289 lb/in³ ASTM D1505
Specific Gravity1.32 g/cc0.0477 lb/in³ ASTM D792

Mechanical Properties
Hardness, Rockwell R100100 ASTM D785
Hardness, Shore D8383 Instantaneous; ASTM D2240
Tensile Strength, Yield41.4 MPa6000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.72 GPa394 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.63 GPa382 ksi ASTM D790
Flexural Strength78.4 MPa11370 psi ASTM D790
Izod Impact, Notched12.4 J/cm23.2 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)65 °C149 °F Unannealed, 0.125 in bars; ASTM D648

Optical Properties
Transmission, Visible81 %81 % 33.5 mils, 400 nm
Transmission, Visible86.5 %86.5 % 33.5 mils, 700 nm

Processing Properties
Melt Temperature199 - 213 °C390 - 415 °F Blow Molding

Descriptive Properties
Product FormPellets 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。