PolyOne Geon® 2192 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Transparent
- Medium Impact
- High Gloss
Applications: - FDA (Food Contact)
- Bottles
Market: Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
Specific Gravity | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Rockwell R | 100 | 100 | ASTM D785 |
Hardness, Shore D | 81 | 81 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 2.4 GPa | 347.4 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.81 GPa | 407 ksi | ASTM D790 |
Flexural Strength | 78.6 MPa | 11400 psi | ASTM D790 |
Izod Impact, Notched | 1.12 J/cm | 2.1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 67.8 °C | 154 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 81 % | 81 % | 33.0 mils, 400 nm |
Transmission, Visible | 84 % | 84 % | 33.0 mils, 700 nm |
Processing Properties |
|
Melt Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|