PolyOne Geon® 2710 CLR 9500 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
The formula has a green blue tint Description/Features: - High Impact
- High Flow
- Transparent
- High Gloss
- UV Stabilized
Applications: - FDA (Food Contact)
- Hotel Amenities
- Mouthwash
- Cosmetics
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82 | 82 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 44.4 MPa | 6440 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 2.36 GPa | 341.6 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Flexural Strength | 77.3 MPa | 11210 psi | ASTM D790 |
Izod Impact, Notched | 1.01 J/cm | 1.9 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 20 °C | 68 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 69 % | 69 % | 30.0 mils, 400 nm |
Transmission, Visible | 85 % | 85 % | 30.0 mils, 700 nm |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|