PolyOne Geon® 3201-xx05D Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized per QMFZ2
- UL 60°C
- UL 94 HB
- Flame Retardant
Applications: - Apparatus & Cord Molding
- Plug Molding
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 62 | 62 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 375 % | 375 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | -50 °C | -58 °F | ASTM D746 |
Flammability, UL94 | HB | HB | All Colors; 0.059 in.; PolyOne Internal |
Processing Properties |
|
Melt Temperature | 154 - 160 °C | 310 - 320 °F | Molding |
Descriptive Properties | |
Product Form | Pellets/Cubes | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|