PolyOne Geon® 78812 Vinyl Compound - Flexible (FPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Medium Gloss

Applications:

  • General Purpose

Market:

  • Automotive

Processing Method:

  • Extrusion and Molding

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.24 g/cc0.0448 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A5858 15 sec; ASTM D2240
Hardness, Shore A6363 Instantaneous; ASTM D2240
Tensile Strength, Ultimate11.4 MPa1650 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Strength, Ultimate4.14 MPa600 psi Type 4 - Flexibles, 2 in/min, 100% in/in; ASTM D638
Elongation at Break400 %400 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength31.6 kN/m180 pli Die C (graves), 20 in/min; ASTM D624
Clash Berg Modulus0.031 GPa4.5 ksi -31°F (-35°C); ASTM D1043

Thermal Properties
Brittleness Temperature-45 °C-49 °F ASTM D746
Clash Berg Stiffness Temperature-45 °C-49 °F 45,000 psi; ASTM D1043

Processing Properties
Melt Temperature168 - 177 °C335 - 350 °F Extrusion

Descriptive Properties
Automotive ApprovalDaimlerChrysler, MS-DC225 
Product FormPellets 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。