PolyOne Geon® 86155 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Processing Method: Disclaimer: NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is “For foods of high water content only”. This material is also listed under NSF Std. 61. This listing covers many uses and restrictions may apply depending on the application. It is the customer's responsibility to ensure that the compound is suitable for its intended application. Please contact us to review the suitability of specific products in specific applications. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 84 | 84 | 15 sec; ASTM D2240 |
Hardness, Shore A | 90 | 90 | Instantaneous; ASTM D2240 |
Tensile Strength, Ultimate | 10.7 MPa | 1550 psi | Type 4 - Flexibles, 20 in/min, 100% in/in; ASTM D638 |
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 400 % | 400 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tear Strength | 76.3 kN/m | 435 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties |
|
Brittleness Temperature | -27 °C | -16.6 °F | ASTM D746 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|