PolyOne Geon® 8700A Vinyl Compound - Rigid (RPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Excellent Dimensional Stability
  • High Melt Strength
  • UL 94 V0
  • UL 94 5VA
  • CSA V0
  • NSF STD 51

Applications:

  • General Purpose
  • Custom Profiles-Complex
  • Custom Profiles-Thick wall
  • Beltline Moldings

Market:

  • Automotive

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: Automotive OEM approval(s).
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.
Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.38 g/cc0.0499 lb/in³ ASTM D792

Mechanical Properties
Hardness, Rockwell R111111 ASTM D785
Hardness, Shore D7878 15 sec; ASTM D2240
Tensile Strength, Yield42.7 MPa6200 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.69 GPa390 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.62 GPa380 ksi ASTM D790
Flexural Strength75.8 MPa11000 psi ASTM D790
Compressive Strength55.8 MPa8100 psi ASTM D695
Dart Drop Total Energy37.4 J/cm0.07 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy37.4 J/cm0.07 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.587 J/cm1.1 ft-lb/in Method A, Compression Molded, 0.125 in bars, 0°F (-18°C); ASTM D256
Izod Impact, Notched0.854 J/cm1.6 ft-lb/in Method A, Compression Molded, 0.125 in bars, 32°F (0°C); ASTM D256
Izod Impact, Notched9.08 J/cm17 ft-lb/in Method A, Compression Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Electrical Properties
Dielectric Constant3.33.3 1,000 Hz; ASTM D150
Dielectric Constant3.93.9 60 Hz; ASTM D150
Dielectric Strength27.2 kV/mm690 V/mil ASTM D149
Dissipation Factor0.0290.029 60 Hz, 86°F (30°C), 24 hrs; ASTM D150
Dissipation Factor0.040.04 1,000 Hz, 86°F (30°C), 24 hrs; ASTM D150

Thermal Properties
CTE, linear 68°F66.6 µm/m-°C37 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)72.8 °C163 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0V-0 All Colors; 0.028 in.
Flammability, UL94V-0V-0 All Colors; 0.034 in.
Flammability, UL9477 All Colors; 0.059 in.

Processing Properties
Melt Temperature179 - 182 °C355 - 360 °F Extrusion

Descriptive Properties
Automotive ApprovalGeneral Motors, GMP 7001M PVC 
Cell Classification D178416344 ASTM D1784
Ease of SizingExcellent 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。