PolyOne Geon® 87018 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Processing Method: PolyOne First ChoiceDisclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. NOTE: Physical Properties were measured on flat cellular profiles with a 0.72 specific gravity natural compound. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 0.6 - 0.75 g/cc | 0.0217 - 0.0271 lb/in³ | Cellular; ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 73 | 73 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 14.8 MPa | 2140 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 1.06 GPa | 154 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 1.36 GPa | 197 ksi | ASTM D790 |
Flexural Strength | 30.2 MPa | 4380 psi | ASTM D790 |
Dart Drop Total Energy | 10.7 J/cm | 0.02 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 10.7 J/cm | 0.02 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 0.32 J/cm | 0.6 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 0.481 J/cm | 0.9 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 0.961 J/cm | 1.8 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 55.8 µm/m-°C | 31 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 56.1 °C | 133 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 182 - 193 °C | 360 - 380 °F | Extrusion |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|