PolyOne Geon® 87263 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior-Weatherable Natural Base
- UL 94 V0
Applications: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of unpigmented compounds or so-called natural compounds generally is inferior to pigmented compounds. Unpigmented weatherable compounds may also contain non-pigment ingredients which can interact unpredictably with pigments to produce unexpected weathering results. Therefore, in applications where processors or customers would like to use an unpigmented compound, or add their own pigment package, it is the customer’s responsibility to determine whether or not the weathering performance after pigmenting is acceptable in their specific end-use application. Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.4 g/cc | 0.0506 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82.3 | 82.3 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 47.2 MPa | 6850 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 2.9 GPa | 420.5 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.83 GPa | 411 ksi | ASTM D790 |
Flexural Strength | 84 MPa | 12190 psi | ASTM D790 |
Dart Drop Total Energy | 58.7 J/cm | 0.11 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 58.7 J/cm | 0.11 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 9.82 J/cm | 18.4 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 10.7 J/cm | 20 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 10.8 J/cm | 20.2 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 64.8 µm/m-°C | 36 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 182 - 193 °C | 360 - 380 °F | |
Descriptive Properties | |
Cell Classification D1784 | 16354 | ASTM D1784 |
Cell Classification D4216 | 14143431 | ASTM D4216 |
Ease of Sizing | Good | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|