PolyOne Geon® 87416 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior-Excellent Weatherability
- High Impact
- Broad Color Palette
- UL 94 V0
- CSA V0
- CSA A440
- AAMA 303
Applications: - Custom Profiles
- Custom Profiles-Thin wall
- Window Components
Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82 | 82 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 2.48 GPa | 360 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Dart Drop Total Energy | 53.4 J/cm | 0.1 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 176 J/cm | 0.33 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 1.55 J/cm | 2.9 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 1.6 J/cm | 3 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 1.6 J/cm | 3 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 61.2 µm/m-°C | 34 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Flammability, UL94 | V-0 | V-0 | All Colors; 0.03 in. |
Flammability, UL94 | V-0 | V-0 | All Colors; 0.039 in. |
Processing Properties |
|
Melt Temperature | 182 - 193 °C | 360 - 380 °F | Extrusion |
Descriptive Properties | |
AAMA 303 | Pass | ASTM D4726 |
Automotive Approval | General Motors, GMP 7001M PVC | |
Cell Classification D1784 | 13344 | ASTM D1784 |
Cell Classification D4216 | 13143233 | ASTM D4216 |
Ease of Sizing | Acceptable | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|