PolyOne Geon® 87431 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - NSF Type I
- PPI-2000 psi Rated
- Normal Impact
- Low Flow
Market: - Fittings (Potable Water, DWV, etc.)
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.002 - 0.005 cm/cm | 0.002 - 0.005 in/in | ASTM D955 |
Mechanical Properties |
|
Hardness, Shore D | 88 | 88 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 53.1 MPa | 7700 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Tensile Modulus | 3.07 GPa | 445 ksi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Flexural Modulus | 3.31 GPa | 480 ksi | ASTM D790 |
Flexural Strength | 93.8 MPa | 13600 psi | ASTM D790 |
Izod Impact, Notched | 0.481 J/cm | 0.9 ft-lb/in | Method A, Injection Molded, 0.250 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | Unannealed, 0.250 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 202 - 204 °C | 395 - 400 °F | Molding |
Descriptive Properties | |
Cell Classification D1784 | 12464 | ASTM D1784 |
NSF | Acceptable | Std 14-Plastic Piping Comp. |
NSF | Acceptable | Std 61-Drinking Water Appl. |
Product Form | Pellets/Cubes | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|