PolyOne Geon® 87560 Vinyl Compound - Rigid (RPVC)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Transparent

Processing Method:

  • Extrusion-Sheet
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.33 g/cc0.048 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D8383 15 sec; ASTM D2240
Tensile Strength, Yield51.8 MPa7520 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.73 GPa396 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.92 GPa424 ksi ASTM D790
Flexural Strength86.2 MPa12500 psi ASTM D790
Dart Drop Total Energy58.7 J/cm0.11 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy198 J/cm0.37 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.534 J/cm1 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.747 J/cm1.4 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.854 J/cm1.6 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F72 µm/m-°C40 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)65 °C149 °F Unannealed, 0.125 in bars; ASTM D648

Processing Properties
Melt Temperature191 - 204 °C375 - 400 °F Extrusion

Descriptive Properties
Cell Classification D178412443 ASTM D1784
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。