PolyOne Geon® 90049 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior
- High Gloss
- Transparent
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
| Collected Volatile Condensable Material | 0.43 % | 0.43 % | Emery, 221°F (105°C), 0.075 in; ASTM D1203B |
Mechanical Properties |
|
| Hardness, Shore A | 83 | 83 | 15 sec; ASTM D2240 |
| Tensile Strength, Ultimate | 19.2 MPa | 2785 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 324 % | 324 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Tear Strength | 63.3 kN/m | 361 pli | Die C (graves), 2 in/min; ASTM D1004 |
Descriptive Properties | |
| Automotive Approval | General Motors, GMP.PVC.010 | Pass |
| Automotive Approval | DaimlerChrysler, MS-DC211-B | Pass |
| Fungal Resistance | Pass | ASTM G21 |
| Low Temperature Flexibility (LTF) | Pass | 12 mm, -20°F (-29°C), 4 hrs, 0.020 in |
| Product Form | Pellets | |
| Xenon Weatherometer - Exterior | Pass | 2,500 kJ/m², Natural, dE*; SAE J1960 |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|